Polymer Property : Izod Impact, Unnotched = 13.7 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 7.30 J/cm
13.7 ft-lb/in
ASTM D256
Solvay Specialty Polymers Ixef® 1028 Polyarylamide (PARA)  (discontinued **)
Ixef 1028 is a laser printable, 50% glass-fiber reinforced polyarylamide which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance. - Black: Ixef 1028..
Izod Impact, Unnotched 7.31 J/cm
13.7 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRILOY RF203AXH PA 66
LNP* LUBRILOY* RF203AXH is a compound based on Nylon 66 resin containing 15% Glass Fiber, Proprietary Lubricant. Added features of this material include: Wear Resistant, Healthcare.
Izod Impact, Unnotched 7.30 J/cm
13.7 ft-lb/in
ASTM D4812
SABIC Innovative Plastics Valox® 412 PBT (Europe-Africa-Middle East)
VALOX 412 is 20% glass reinforced PBT injection moulding resin. Applications: Spotlights, appliance housings and handles.
Izod Impact, Unnotched 7.30 J/cm
13.7 ft-lb/in
ASTM D4812
SABIC Innovative Plastics Valox® 865 PBT (Europe-Africa-Middle East)
VALOX 865 is a 30% glass fibre reinforced, non blooming flame retardant PBT+PET blend with an excellent surface appearance. Applications: External housings, steam irons, appliance housings and light..
Izod Impact, Unnotched 7.32 J/cm
13.7 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON DX09315C PC (Asia Pacific)
LNP* Stat-Kon* DX09315C is carbon fiber filled polycarbonate composite with good flow ability, and high level of cleanliness for the most demanding application. A unique feature of this material is ..
Izod Impact, Unnotched 7.32 J/cm
13.7 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON REL33 PA 66
LNP STAT-KON* REL33 is a compound based on Nylon 66 resin containing 15% Carbon Fiber, 15% PTFE. Added features of this material include: Electrically Conductive, Wear Resistant.
Izod Impact, Unnotched 7.29 J/cm
13.7 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP DX06412H PC
LNP* THERMOCOMP* DX06412H is a compound based on Polycarbonate resin containing 30% Glass Fiber. Added features of this material include: Easy Molding, Mold Release.
Izod Impact, Unnotched 7.29 J/cm
13.7 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP DX06412H PC (Asia Pacific)
LNP* Thermocomp* DX06412H is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release.
Izod Impact, Unnotched 7.29 J/cm

@Temperature 23.0 °C
13.7 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics LNP Thermocomp KB002 Acetal Copoly
LNP* Thermocomp* KB002 is a compound based on Acetal Copolymer resin containing Glass Bead.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Unnotched 7.31 J/cm
13.7 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP RF006EXZ PA 66
LNP THERMOCOMP* RF006EXZ is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of this material include: Easy Molding.
Izod Impact, Unnotched 7.29 J/cm

@Temperature 23.0 °C
13.7 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics LNP Thermocomp KB002 Acetal Copoly (Asia Pacific)
LNP* Thermocomp* KB002 is a compound based on Acetal Copolymer resin containing Glass Bead.This data was supplied by SABIC-IP for the Asia Pacific region.
Izod Impact, Unnotched 7.31 J/cm
13.7 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP RF006ESZ PA 66
LNP THERMOCOMP* RF006ESZ is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized.
Izod Impact, Unnotched 7.29 J/cm
13.7 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP RF0069XZ PA 66
LNP THERMOCOMP* RF0069XZ is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of this material include: Flame Retardant.