Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 7.00 J/cm | 13.1 ft-lb/in | ASTM D4812 |
Premix Premi-Glas® 1201-20 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1201-20 is a fiberglass reinforced thermoset sheet molding compound for sanitary ware applications such as shower bases and surrounds, bathtubs and vanity tops.Key features and benefits.. |
|||
Izod Impact, Unnotched | 7.00 J/cm | 13.1 ft-lb/in | ASTM D4812 |
Premix Premi-Glas® 2200-15 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2200-15 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Izod Impact, Unnotched | 7.00 J/cm | 13.1 ft-lb/in | ASTM D4812 |
Premix Premi-Glas® 2203-15 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2203-15 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Izod Impact, Unnotched | 7.00 J/cm | 13.1 ft-lb/in | ASTM D4812 |
Premix Premi-Glas® 2203-15 CR-SX-HT Fiberglass Reinforced Thermoset SMC Premi-Glas® 2203-15 CR-SX-HT is a fiberglass reinforced thermoset sheet molding compound for electrical and flame retardant applications.Key features and benefits are:Enhanced product for higher UL.. |
|||
Izod Impact, Unnotched | 7.00 J/cm | 13.1 ft-lb/in | ASTM D4812 |
Premix Premi-Glas® 2204-15 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2204-15 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Izod Impact, Unnotched | 7.00 J/cm | 13.1 ft-lb/in | ASTM D4812 |
Premix Premi-Glas® 2205-15 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2205-15 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Izod Impact, Unnotched | 7.00 J/cm | 13.1 ft-lb/in | ASTM D4812 |
Premix Premi-Glas® 2206-25 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2206-25 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Non-Halogen FR technology f.. |
|||
Izod Impact, Unnotched | 7.00 J/cm | 13.1 ft-lb/in | ASTM D4812 |
Premix Premi-Glas® 3200-15 Fiberglass Reinforced SMC Description: Premi-Glas® 3200-15 is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal and di.. |
|||
Izod Impact, Unnotched | 7.00 J/cm | 13.1 ft-lb/in | Average value: 7.00 J/cm Grade Count:3 |
Overview of materials for PET + PBT Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "PET + PBT Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Izod Impact, Unnotched | >= 7.00 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
>= 13.1 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa LONOY 3010 Glass Fiber Reinforced PC/PBT Alloy Features:Excellent balance propertiesGood weather resistanceGood size stabilitySmooth surfaceUniform colorApplications:Injection moldingElectric and electronic partsBusiness machine cabinetGarden to.. |
|||
Izod Impact, Unnotched | 7.00 J/cm | 13.1 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Ixef® 1025 Polyarylamide (PARA), 50% Glass Fiber Ixef® 1025 is a 50% glass-fiber reinforced, UV stabilized polyarylamide which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Features: Good Ch.. |
|||
Izod Impact, Unnotched | 7.00 J/cm | 13.1 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Ixef® 1521 Polyarylamide (PARA), 50% Glass Fiber Ixef® 1521 is a 50% glass-fiber reinforced, flame retardant polyarylamide which exhibits high strength and stiffness, outstanding surface gloss, and excellent creep resistance.Features: Flame Ret.. |
|||
Izod Impact, Unnotched | 7.00 J/cm | 13.1 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® IQ8280SF PBT+PET Valox iQ8280SF resin is an environmentally responsible, low carbon footprint, and sustainable resin. Valox iQ8280SF resin offer Super High Flow characteristics combined with high modulus and excell.. |
|||
Izod Impact, Unnotched | 7.00 J/cm | 13.1 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® IQ8280SF PBT+PET (Asia Pacific) Valox iQ8280SF resin is an environmentally responsible, low carbon footprint, and sustainable resin. Valox iQ8280SF resin offer Super High Flow characteristics combined with high modulus and excell.. |
|||
Izod Impact, Unnotched | 7.00 J/cm | 13.1 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® IQ8280SF PBT+PET (Europe-Africa-Middle East) Valox iQ8280SF resin is an environmentally responsible, low carbon footprint, and sustainable resin. Valox iQ8280SF resin offer Super High Flow characteristics combined with high modulus and excell.. |
|||
Izod Impact, Unnotched | 7.01 J/cm | 13.1 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP KF005 Acetal Copolymer LNP THERMOCOMP* KF005 is a compound based on Acetal Copolymer resin containing 25% Glass Fiber. Added features of this material include: Chemically Coupled. |
|||
Izod Impact, Unnotched | 6.97 J/cm @Temperature 23.0 °C |
13.1 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Lubricomp XL004 Amorphous Polyamide LNP* Lubricomp* XL-4040 is a compound based on Amorphous Nylon, containing PTFE.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched | 6.99 J/cm | 13.1 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Hiloy® 413 Polyester - PBT, Glass Reinforced Data provided by the manufacturer, ComAlloy International Company.33% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Unnotched | 6.99 J/cm | 13.1 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Hiloy® 433 Glass Reinforced, PBT Alloy Data provided by the manufacturer, ComAlloy International Company.45% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Unnotched | 6.99 J/cm | 13.1 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Aqualoy® 150 Polypropylene, Glass Reinforced, Chemically Coupled NSF Data provided by the manufacturer, ComAlloy International Company.50% Glass Reinforced. In Aqualoy® materials, carefully selected base resins and proprietary additives meld hydrolytic stability an.. |