Izod Impact, Unnotched 10.89 J/cm
20.40 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP PFL36 PA 6
LNP* LUBRICOMP* PFL36 is a compound based on Nylon 6 resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant.
Izod Impact, Unnotched 10.89 J/cm
20.40 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP PFL36 PA 6 (Asia Pacific)
LNP* Lubricomp* PFL36 is a compound based on Nylon 6 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.
Izod Impact, Unnotched 10.89 J/cm
20.40 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP RF008ESY PA 66
LNP THERMOCOMP* RF008ESY is a compound based on Nylon 66 resin containing 40% Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized.
Izod Impact, Unnotched 10.89 J/cm
20.40 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOTUF PX06417 PA 6
LNP THERMOTUF* PX06417 is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.