Polymer Property : Izod Impact, Unnotched = 10.6 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 5.64 J/cm
10.6 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP KL002 Acetal Copoly
LNP* LUBRICOMP* KL002 is a compound based on Acetal Copolymer resin containing 10% PTFE. Added feature of this material is: Wear Resistant.
Izod Impact, Unnotched 5.64 J/cm
10.6 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP KL002 Acetal Copoly (Asia Pacific)
LNP* Lubricomp* KL002 is a compound based on Acetal Copolymer resin containing PTFE. Added features of this material include: Internally Lubricated.
Izod Impact, Unnotched 5.64 J/cm
10.6 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP KL002L Acetal
LNP* LUBRICOMP* KL002L is a compound based on Acetal Copolymer resin containing 10% PTFE. Added features of this grade include: Wear Resistant, Low Extractible.
Izod Impact, Unnotched 5.65 J/cm
10.6 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP ML004LS PP
LNP* LUBRICOMP* ML004LS is a compound based on Polypropylene resin containing 20% PTFE. Added features of this matLNP* Lubricomp* ML004LS is a compound based on Polypropylene resin containing PTFE...
Izod Impact, Unnotched 5.68 J/cm
10.6 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP JF008E PES
LNP* THERMOCOMP* JF008E is a compound based on Polyethersulfone containing 40% Glass Fiber. Characteristics of this grade are: Easy Molding.
Izod Impact, Unnotched 5.66 J/cm
10.6 ft-lb/in
ASTM D256
A. Schulman ComAlloy Comtuf® 413 Glass Reinforced, Polycarbonate/Polyester Alloy, UL
Data provided by the manufacturer, ComAlloy International Company.20% Glass Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been int..
Izod Impact, Unnotched 5.68 J/cm
10.6 ft-lb/in
63.5*12.7*3.2mm, Cut; ASTM D4812
SABIC Innovative Plastics SABIC PPCOMPOUND G3230A PP
SABIC® PPcompound G3230A is a general purpose, 30% glass filled, chemically coupled, heat stabilized homopolymer polypropylene compound. The IMDS ID is 109612410