Polymer Property : Izod Impact, Unnotched = 1.85 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 1.85 J/cm
3.47 ft-lb/in
ASTM D256
A. Schulman POLYFORT™ FPP 1080 Glass Fiber-Reinforced Homopolymer Polypropylene
DescriptionPolyfort® FPP 1080 is a 20% fiber-reinforced homopolymer polypropylene with excellent strength and heat resistance. Information provided by A. Schulman.
Izod Impact, Unnotched 1.85 J/cm
3.47 ft-lb/in
ASTM D256
A. Schulman POLYFORT™ FPP 1080 Glass Fiber-Reinforced Homopolymer Polypropylene
DescriptionPolyfort® FPP 1080 is a 20% fiber-reinforced homopolymer polypropylene with excellent strength and heat resistance. Information provided by A. Schulman.
Izod Impact, Unnotched 1.85 J/cm
3.47 ft-lb/in
ASTM D256
A. Schulman POLYFORT™ FPP 1080 Glass Fiber-Reinforced Homopolymer Polypropylene
DescriptionPolyfort® FPP 1080 is a 20% fiber-reinforced homopolymer polypropylene with excellent strength and heat resistance. Information provided by A. Schulman.
Izod Impact, Unnotched 1.85 J/cm
3.47 ft-lb/in
ASTM D256
A. Schulman POLYFORT™ FPP 1080 Glass Fiber-Reinforced Homopolymer Polypropylene
DescriptionPolyfort® FPP 1080 is a 20% fiber-reinforced homopolymer polypropylene with excellent strength and heat resistance. Information provided by A. Schulman.
Izod Impact, Unnotched 1.85 J/cm
3.47 ft-lb/in
ASTM D256
A. Schulman POLYFORT™ FPP 1080 Glass Fiber-Reinforced Homopolymer Polypropylene
DescriptionPolyfort® FPP 1080 is a 20% fiber-reinforced homopolymer polypropylene with excellent strength and heat resistance. Information provided by A. Schulman.
Izod Impact, Unnotched 1.85 J/cm
3.47 ft-lb/in
ASTM D256
A. Schulman POLYFORT™ FPP 1080 Glass Fiber-Reinforced Homopolymer Polypropylene
DescriptionPolyfort® FPP 1080 is a 20% fiber-reinforced homopolymer polypropylene with excellent strength and heat resistance. Information provided by A. Schulman.