Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact Notched | 1.25 J | 0.920 ft-lb | ASTM D256A |
ExxonMobil PP4792E1 Polymer Grade for Oriented Film Product Description: Easy processing grade primarily for oriented film applications.Availability: North America Features:MetalizableUses: Oriented FilmPackagingTapeProcessing Method: Film Extrusi.. |