Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Creep Strength | 30.0 MPa @Time 3.60e+6 sec |
4350 psi @Time 1000 hour |
in water at 95°C |
BASF Ultrason S 2010 G6 30% Glass Filled PSU Ultrason S 2010 G6 is a 30% glass reinforced, medium viscosity injection molding PSU grade with high rigidity and strength. |
|||
Creep Strength | 30.0 MPa @Time 3.60e+6 sec |
4350 psi @Time 1000 hour |
in water at 95°C |
BASF Ultrason E 2010 G6 30% Glass Filled PES Ultrason E 2010 G6 is a 30% glass reinforced, medium viscosity injection molding PES grade with high rigidity and strength. |
|||
Creep Strength | 30.0 MPa @Time 36000 sec |
4350 psi @Time 10.0 hour |
in water at 95°C |
BASF Ultrason E 3010 PES Ultrason E 3010 is an unfilled, higher viscosity injection molding and extrusion PES grade, tougher and with improved chemical resistance. |
|||
Creep Strength | 30.0 MPa @Time 3.60e+7 sec |
4350 psi @Time 10000 hour |
in water at 95°C |
BASF Ultrason® P 3010 PPSU Unreinforced Polyphenylsulfone Description: Medium viscosity injection-molding and extrusion grade with good toughness and chemical resistance (stress crack resistance), resistant against superheated steam. The property profile m.. |