Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 19.5 J/cm² @Temperature -20.0 °C |
92.8 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eU |
Borealis Daplen™ ED135AI TPO Compound Daplen ED135AI is a 10% mineral filled grade intended for injection molding. ED135AI offers very good balance in stiffness/impact strengthDaplen ED135AI has been developed especially for the car in.. |