Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 1.00 - 9.50 J/cm² | 4.76 - 45.2 ft-lb/in² | Average value: 7.56 J/cm² Grade Count:25 |
Overview of materials for Polyphthalamide (PPA), 50% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 50% Glass Fiber Reinforced". Each property range of values reported is minimum and maxi.. |
|||
Charpy Impact Unnotched | 2.50 - 9.50 J/cm² | 11.9 - 45.2 ft-lb/in² | Average value: 5.48 J/cm² Grade Count:19 |
Overview of materials for Nylon 66/6, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are incl.. |
|||
Charpy Impact Unnotched | 2.20 - 9.50 J/cm² | 10.5 - 45.2 ft-lb/in² | Average value: 5.15 J/cm² Grade Count:32 |
Overview of materials for Nylon 66, 10% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Carbon Fiber Filled". Specific grades with carbon fiber content between 5% and 14% are inc.. |
|||
Charpy Impact Unnotched | 6.00 - 9.50 J/cm² @Temperature -30.0 - 30.0 °C |
28.6 - 45.2 ft-lb/in² @Temperature -22.0 - 86.0 °F |
Average value: 7.83 J/cm² Grade Count:20 |
Overview of materials for Nylon 12, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. .. |
|||
Charpy Impact Unnotched | 1.80 - 9.50 J/cm² | 8.57 - 45.2 ft-lb/in² | Average value: 4.38 J/cm² Grade Count:4 |
Overview of materials for Nylon 66, 40% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Carbon Fiber Filled". Specific grades with carbon fiber content between 35% and 44% are in.. |