Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 8.70 J/cm² @Temperature 23.0 °C |
41.4 ft-lb/in² @Temperature 73.4 °F |
Injection Molded; ISO 179 |
PolyOne Bergamid™ B70 G45 BK Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Charpy Impact Unnotched | 8.70 J/cm² @Temperature 23.0 °C |
41.4 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
PolyOne Bergamid™ B70 UF V2 Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Charpy Impact Unnotched | 8.70 - 103 J/cm² @Temperature -30.0 - -30.0 °C |
41.4 - 490 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 68.3 J/cm² Grade Count:6 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Glass Filled". Each property range of values reported is minimum .. |
|||
Charpy Impact Unnotched | 8.70 J/cm² @Temperature -30.0 °C |
41.4 ft-lb/in² @Temperature -22.0 °F |
|
Ineos ABS Lustran® 248 Key Features:UnfilledSuitable processing methods:Injection molding |
|||
Charpy Impact Unnotched | 8.70 J/cm² @Temperature 23.0 °C |
41.4 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1eU |
Gromax BTG25-FN09N1 Nylon 6 25% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Charpy Impact Unnotched | 8.70 J/cm² | 41.4 ft-lb/in² | ISO 179/1eU |
Solvay TECHNYL® A 218 V25 Black 21 N PA66, 25% glass fiber, Conditioned Description: TECHNYL® A 218 V25 is a polyamide 66, reinforced with 25% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Charpy Impact Unnotched | 8.70 J/cm² | 41.4 ft-lb/in² | ISO 179/1eU |
Solvay TECHNYL® A 218G2 V30 Black 34N PA66, 30% glass fiber, DRY Description: TECHNYL® A 218G2 V30 Black 34N is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product is available in black color. Benefits: This .. |
|||
Charpy Impact Unnotched | 8.70 J/cm² @Temperature -30.0 °C |
41.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Styrolution Styrolux 3G55 SBC Styrolux 3G55 is a thermoplastic styrene-butadiene block copolymer which is suitable for film and sheet extrusion, and thermoforming. It offers and outstanding combination of crystal clarity and ex.. |
|||
Charpy Impact Unnotched | 8.70 J/cm² @Temperature -30.0 °C |
41.4 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 179/1eU |
DuPont Performance Polymers Zytel® 80G25HS BK117 Nylon 66
(Unverified Data**) 25% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G25HS BK117 is a 25% glass fiber reinforced toughened heat stabilized black polyamide 66 resin for injection molding.Information p.. |
|||
Charpy Impact Unnotched | 8.70 J/cm² @Temperature -30.0 °C |
41.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
BASF Ultramid® 1603-2 NF2004 43% Glass Filled PA66 (Conditioned) Ultramid 1603-2 NF2004 is a 43% glass reinforced, heat stabilized injection molding nylon 6/6 with the highest level of glass reinforcement for maximum strength and stiffness. |
|||
Charpy Impact Unnotched | 8.70 J/cm² @Temperature -30.0 °C |
41.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Lubrizol ESTALOC® 59003 Ester-Type, Reinforced Engineering Thermoplastic (European Grade) Description: Estaloc® RETP (Reinforced Engineering Thermoplastic) is a tough, dimensionally stable, abrasion-resistant thermoplastic that withstands demanding environments. Developed as an extensio.. |