Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 7.60 J/cm² | 36.2 ft-lb/in² | ISO 179/1eU |
Solvay Specialty Polymers Amodel® AT-6115 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-6115 HS is a 15% glass-fiber reinforced, toughened grade of polyphthalamide (PPA) resin designed to possess more elongation than other 15% glass-fiber reinforced grades of Amodel resin. Th.. |
|||
Charpy Impact Unnotched | 7.60 - 10.5 J/cm² @Temperature -30.0 - 30.0 °C |
36.2 - 50.0 ft-lb/in² @Temperature -22.0 - 86.0 °F |
Average value: 8.93 J/cm² Grade Count:8 |
Overview of materials for Nylon 66/6, 60% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 60% Glass Fiber Reinforced". Specific grades with glass content between 55% and 64% are incl.. |
|||
Charpy Impact Unnotched | 7.60 J/cm² | 36.2 ft-lb/in² | Type 1, Edgewise; ISO 179 |
Solvay Specialty Polymers Amodel® AS-1933 HS Polyphthalamide (PPA), 33% Glass Fiber Amodel® AS-1933 HS is a 33% glass reinforced grade of polyphthalamide (PPA) resin developed specifically for improved performance in a 50/50 ethylene glycol and water environment. This material e.. |
|||
Charpy Impact Unnotched | 7.60 J/cm² | 36.2 ft-lb/in² | Type 1, Edgewise; ISO 179 |
Solvay Specialty Polymers Amodel® AT-6115 HS Polyphthalamide (PPA), 15% Glass Fiber (Dry) Amodel® AT-6115 HS is a 15% glass-fiber reinforced, toughened grade of polyphthalamide (PPA) resin designed to possess more elongation than other 15% glass-fiber reinforced grades of Amodel resin.. |
|||
Charpy Impact Unnotched | 7.60 J/cm² @Temperature -20.0 °C |
36.2 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eU |
Borealis Daplen™ EE260AE Scratch Resistant Polypropylene Compound Daplen EE206AE is a 20% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen EE206AE is optimized to provide excellent scratch resistance on gained and unpai.. |
|||
Charpy Impact Unnotched | 7.60 J/cm² @Temperature 30.0 °C |
36.2 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® TSG-60/4 W PA666-GF60 Product description: Grilon TSG-60/4 W is a high heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 60% glass fibers, modified for parts with high thermal demands. Grilon TSG-.. |
|||
Charpy Impact Unnotched | 7.60 J/cm² | 36.2 ft-lb/in² | 50%RH; ISO 179/1eU |
DuPont Performance Polymers Zytel® 80G14A NC010A Nylon 66
(Unverified Data**) 14% Glass Reinforced Toughened Polyamide 66 Zytel 80G14A NC010A is a 14% glass fiber reinforced toughened high flow polyamide 66 resin. It offers outstanding performance in injection molding applica.. |
|||
Charpy Impact Unnotched | 7.60 J/cm² @Temperature -30.0 °C |
36.2 ft-lb/in² @Temperature -22.0 °F |
|
Arkema Group Rilsan® AUM 50 NOIR T6LD Nylon 12, 50% Glass Bead Filled (Dry) Designation ISO 1874-PA12,MHLR,16-020,GB50Rigid grad with glass beads filler (50%) for injection molding. Available color: black. Reinforced light and heat stabilizing agents. Mold-release agent.Goo.. |
|||
Charpy Impact Unnotched | 7.60 J/cm² - NB @Temperature -40.0 - -30.0 °C |
36.2 ft-lb/in² - NB @Temperature -40.0 - -22.0 °F |
Average value: 7.60 J/cm² Grade Count:4 |
Overview of materials for Nylon 6, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, PTFE Filled". Each property range of values reported is minimum and maximum values of appropria.. |
|||
Charpy Impact Unnotched | 7.60 J/cm² | 36.2 ft-lb/in² | 50%RH; ISO 179/1eU |
DuPont Performance Polymers Zytel® 80G14AHS NC010 Nylon 66
(Unverified Data**) 14% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G14AHS NC010 is a 14% glass fiber reinforced toughened high flow heat stabilized polyamide 66 resin. It offers outstanding perform.. |
|||
Charpy Impact Unnotched | 7.60 J/cm² | 36.2 ft-lb/in² | ISO 179/1eU |
Solvay Specialty Polymers Amodel® AS-1933 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1933 HS is a 33% glass reinforced grade of polyphthalamide (PPA) resin developed specifically for improved performance in a 50/50 ethylene glycol and water environment. This material excee.. |