Polymer Property : Charpy Impact Unnotched = 7.20 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 7.20 J/cm²
34.3 ft-lb/in²
flatwise; ISO 179 1fU
Lehmann & Voss LUVOCOM® 1-0935 Polyamide 66, with glass fiber and PTFE, 8-mm-granulate
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec..
Charpy Impact Unnotched 7.20 J/cm²
34.3 ft-lb/in²
ISO 179/1eU
Solvay TECHNYL® A 218G V33 Black 41N PA66, 33% glass fiber, DRY
Description: TECHNYL® A 218G V33 Black 41N is a polyamide 66, reinforced with 33% of glass fiber, heat stabilized, for injection molding. The product is available in black color.Benefits: This pr..
Charpy Impact Unnotched 7.20 J/cm²
34.3 ft-lb/in²
ISO 179/1eU
Solvay TECHNYL® A 21T2 V25 PA66, 25% glass fiber, Conditioned
Description: Flame retardant polyamide 66, reinforced with 25% of glass fiber, heat stabilized, for injection molding.Available in: Asia Pacific, Europe, Latin America and North AmericaProduct Appl..
Charpy Impact Unnotched 7.20 J/cm²

@Temperature 23.0 °C
34.3 ft-lb/in²

@Temperature 73.4 °F
ISO 179
CP-Polymer-Technik Wellamid® 6600 CF20 HWCP 20% Carbon Fiber Nylon 66, Heat Stabilized, Conditioned
Information provided by CP-Polymer-Technik GmbH & Co. KG
Charpy Impact Unnotched 7.20 J/cm²
34.3 ft-lb/in²
ISO 179
Chi Mei Kibiton® PB-5903 SBC
High transparency, high toughness, PS Impact modifier
Charpy Impact Unnotched 7.20 J/cm²

@Temperature 23.0 °C
34.3 ft-lb/in²

@Temperature 73.4 °F
EN ISO 179
Ensinger TECASINT 4011 Polyimide, Yellow (PI)
TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel..