Polymer Property : Charpy Impact Unnotched = 48.5 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 10.2 J/cm²

@Temperature -30.0 °C
48.5 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eU
SABIC Innovative Plastics Lexan® HFD4271 PC
Lexan* HFD4271 is a 10% glass filled, high flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4271 has enhanced mold release, impact ductility..
Charpy Impact Unnotched 10.2 J/cm²

@Temperature -30.0 °C
48.5 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eU
SABIC Innovative Plastics Lexan® HFD4271 PC (Asia Pacific)
Lexan* HFD4271 is a 10% glass filled, high flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4271 has enhanced mold release, impact ductility..
Charpy Impact Unnotched 10.2 J/cm²
48.5 ft-lb/in²
ISO 179/1eU
Solvay TECHNYL® C 216 V35 Black Z PA6, 35% glass fiber, DRY
Description: Polyamide PA6 , reinforced with 35 % of glass fiber, for injection molding.Available in: North AmericaProduct Applications: It has good mechanical properties, it is used in all sectors ..
Charpy Impact Unnotched 10.2 J/cm²

@Temperature -30.0 °C
48.5 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Solvay TECHNYL® C 246SI V30 PA6, 30% glass filled, Conditioned
Description: Polyamide 6, reinforced with 30 % of glass fiber, with high impact resistance, for injection molding.Available in: Asia Pacific , Europe and North AmericaProduct Applications: Having go..
Charpy Impact Unnotched 10.2 J/cm²
48.5 ft-lb/in²
ISO 179/1eU
Borealis Xmod™ BG055AI High Stiffness Polypropylene for Injection Molding Applications
Xmod BG055AI is a high melt flow polypropylene with increased crystallinity, intended for injection molding. Xmod BG055AI is a very easy flowing material with a good balance between impact strength..
Charpy Impact Unnotched 10.2 J/cm²
48.5 ft-lb/in²
ISO 179-1
Unitika B2040G50 PA66, 50% Glass Fiber Reinforced, Conditioned
Information provided by Unitika Ltd.
Charpy Impact Unnotched 10.2 J/cm²
48.5 ft-lb/in²
Arkema Group Rilsan® BZM 8 NOIR TL Nylon 11, 8% Glass Fiber Filled (Conditioned)
Designation ISO 1874-PA11,MHL,18-020,GF8Rigid grade with glass fiber (8%) filler for injection molding. Available color: black. Light and heat stabilized.Rigidity. Outstanding compromise between goo..
Charpy Impact Unnotched 10.2 J/cm²

@Temperature 23.0 °C
48.5 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Akro-Plastic Akromid® A3 GF 35 (2421) PA 6.6 Conditioned, 35% Glass Filled
AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat..
Charpy Impact Unnotched 10.2 J/cm²
48.5 ft-lb/in²
ISO 179
BASF Ultramid® B3ZG7 OSI BK23273 35% Glass Filled PA6 (Dry)
Ultramid B3ZG7 OSI BK23273 is a 35% glass reinforced, pigmented black, heat stabilized, impact modified PA6 injection molding grade. It was developed to meet demanding mechanical and chemical requi..
Charpy Impact Unnotched 10.2 J/cm²

@Temperature -30.0 °C
48.5 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eU
SABIC Innovative Plastics Lexan® HFD4271 PC (Europe-Africa-Middle East)
Lexan* HFD4271 is a 10% glass filled, high flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4271 has enhanced mold release, impact ductility..