Polymer Property : Charpy Impact Unnotched = 4.00 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 1.70 - 4.00 J/cm²

@Temperature -30.0 - -20.0 °C
8.09 - 19.0 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 2.78 J/cm² Grade Count:4
Overview of materials for Polyphthalamide (PPA), 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are..
Charpy Impact Unnotched 1.00 - 4.00 J/cm²
4.76 - 19.0 ft-lb/in²
Average value: 3.00 J/cm² Grade Count:38
Overview of materials for Polycarbonate, Carbon Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximum v..
Charpy Impact Unnotched 1.80 - 4.00 J/cm²

@Temperature -30.0 - 30.0 °C
8.57 - 19.0 ft-lb/in²

@Temperature -22.0 - 86.0 °F
Average value: 2.45 J/cm² Grade Count:4
Overview of materials for Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled". Specific grades with glass content between 35% an..
Charpy Impact Unnotched 4.00 - 4.00 J/cm²

@Temperature -30.0 - -30.0 °C
19.0 - 19.0 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 4.00 J/cm² Grade Count:2
Overview of materials for Liquid Crystal Polymer (LCP), Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Mineral Filled". Each property range of values reported is minimum and max..
Charpy Impact Unnotched 1.20 - 4.00 J/cm²
5.71 - 19.0 ft-lb/in²
Average value: 2.33 J/cm² Grade Count:3
Overview of materials for Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler". Specific grades with glass content between 45%..
Charpy Impact Unnotched 3.00 - 4.00 J/cm²

@Temperature -30.0 - -20.0 °C
14.3 - 19.0 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 3.50 J/cm² Grade Count:8
Overview of materials for Nylon 66, Carbon Fiber/PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Carbon Fiber/PTFE Filled". Each property range of values reported is minimum and maximum value..
Charpy Impact Unnotched 1.50 - 4.00 J/cm²
7.14 - 19.0 ft-lb/in²
Average value: 2.75 J/cm² Grade Count:4
Overview of materials for Nylon 66, Stainless Steel Filled; EMI Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Stainless Steel Filled; EMI Grade". Each property range of values reported is minimum and maxi..
Charpy Impact Unnotched 3.00 - 4.00 J/cm²
14.3 - 19.0 ft-lb/in²
ISO 179
Bulk Molding Compounds tetra-DUR N 4303 Bulk Molding Compound
Mechanical high grade standard product.Typical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion p..
Charpy Impact Unnotched 3.50 - 4.00 J/cm²
16.7 - 19.0 ft-lb/in²
Average value: 3.90 J/cm² Grade Count:5
Overview of materials for Polyphenylene Ether + Styrene-Butadiene Blend, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether + Styrene-Butadiene Blend, Glass Filled". Each property range of values reported is ..
Charpy Impact Unnotched 3.50 - 4.00 J/cm²

@Temperature -30.0 - -30.0 °C
16.7 - 19.0 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 3.90 J/cm² Grade Count:5
Overview of materials for Polyphenylene Ether + Styrene-Butadiene Blend, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether + Styrene-Butadiene Blend, Glass Filled". Each property range of values reported is ..
Charpy Impact Unnotched 1.30 - 4.00 J/cm²
6.19 - 19.0 ft-lb/in²
Average value: 2.85 J/cm² Grade Count:13
Overview of materials for Polybutylene Terephthalate (PBT), Glass + Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass + Mineral Filled". Each property range of values reported is min..
Charpy Impact Unnotched 2.10 - 4.00 J/cm²

@Temperature -30.0 - 30.0 °C
9.99 - 19.0 ft-lb/in²

@Temperature -22.0 - 86.0 °F
Average value: 2.90 J/cm² Grade Count:10
Overview of materials for Polybutylene Terephthalate (PBT), Glass + Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass + Mineral Filled". Each property range of values reported is min..
Charpy Impact Unnotched 3.00 - 4.00 J/cm²
14.3 - 19.0 ft-lb/in²
Average value: 3.72 J/cm² Grade Count:8
Overview of materials for Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant". Each property range of values re..
Charpy Impact Unnotched 2.00 - 4.00 J/cm²

@Temperature -40.0 - -30.0 °C
9.52 - 19.0 ft-lb/in²

@Temperature -40.0 - -22.0 °F
Average value: 3.07 J/cm² Grade Count:6
Overview of materials for Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant". Each property range of values re..
Charpy Impact Unnotched 4.00 - 4.00 J/cm²

@Temperature -30.0 - -30.0 °C
19.0 - 19.0 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 4.00 J/cm² Grade Count:1
Overview of materials for Polysulfone, 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are inc..
Charpy Impact Unnotched 4.00 - 4.00 J/cm²

@Temperature -30.0 - -30.0 °C
19.0 - 19.0 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 4.00 J/cm² Grade Count:1
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Fiber Filled". Each property range of values reported is minimu..