Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 7.40 J/cm² @Temperature 23.0 °C |
35.2 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
PolyOne Bergadur™ PB40 G30 UF UV Polybutylene Terephthalate (PBT) Information provided by PolyOne |
|||
Charpy Impact Unnotched | 7.40 J/cm² @Temperature 23.0 °C |
35.2 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
PolyOne Bergamid™ B650 G/Mi20 UF Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Charpy Impact Unnotched | 7.40 J/cm² @Temperature 23.0 °C |
35.2 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1eU |
Gromax BFG30-AH00B3 Nylon 6 30% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Charpy Impact Unnotched | 7.40 J/cm² | 35.2 ft-lb/in² | |
Arkema Group Rilsan® BZM 23 G9 Nylon 11, 23% Glass Fiber Filled (Conditioned) Designation ISO 1874-PA11,MS,18-040,(G+C)(F+D)(25+05)Rigid grade with glass fiber (23%) and graphite filler for injection molding. Available color: steel black gray. Additive free.Rigidity. Low fric.. |
|||
Charpy Impact Unnotched | 7.40 J/cm² | 35.2 ft-lb/in² | ISO 179 |
BASF Ultradur B 2300 G6 HR BK15116 30% Glass Filled PBT Ultradur B 2300 G6 HR BK15116 is a hydrolysis resistant, pigmented black 30% fiberglass reinforced PBT, exhibiting superior flow characteristics. Designed for improved latch
strength in automotive.. |