Mechanical Properties Metric English Comments
Charpy Impact Unnotched 7.30 J/cm²
34.7 ft-lb/in²
ISO 179/1eU
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resistance..
Charpy Impact Unnotched 7.29 - 7.50 J/cm²

@Temperature -30.0 - -30.0 °C
34.7 - 35.7 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 7.39 J/cm² Grade Count:2
Overview of materials for Nylon 11 with 40% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 40% Glass Fiber Filler". Specific grades with glass content between 35% and 44% are includ..
Charpy Impact Unnotched 7.30 J/cm²
34.7 ft-lb/in²
Type 1, Edgewise; ISO 179
Solvay Specialty Polymers Amodel® A-4133 HH Polyphthalamide (PPA), 33% Glass Fiber (Dry)
Amodel® A-4133 HH is a 33% glass fiber reinforced heat stabilized grade of polyphthalamide (PPA) that has been designed to provide outstanding property retention to thermal oxidative degradation ..
Charpy Impact Unnotched 7.30 J/cm²
34.7 ft-lb/in²
Type 1, Edgewise; ISO 179
Solvay Specialty Polymers Amodel® AE-1133 Polyphthalamide (PPA), 33% Glass Fiber
Amodel® AE-1133 is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) designed to work in the modern automotive electrical environment. It has a high heat deflection temperature, high ..
Charpy Impact Unnotched 7.30 J/cm²
34.7 ft-lb/in²
Type 1, Edgewise; ISO 179
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry)
Amodel® A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resist..
Charpy Impact Unnotched 7.30 J/cm²

@Temperature 23.0 °C
34.7 ft-lb/in²

@Temperature 73.4 °F
ISO 179
CP-Polymer-Technik Wellamid® 6000 GV 20 HWCP 20% Glass Fiber Nylon 6, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
Charpy Impact Unnotched 7.30 J/cm²

@Temperature 30.0 °C
34.7 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
EMS-Grivory Grivory® TSGZ-25/4 PA666-GF25
Information provided by EMS Grivory
Charpy Impact Unnotched 7.30 J/cm²

@Temperature -30.0 °C
34.7 ft-lb/in²

@Temperature -22.0 °F
50%RH; ISO 179/1eU
DuPont Performance Polymers Zytel® 70G30HSL NC010 Nylon 66  (Unverified Data**)
30% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G30HSL NC010 is a 30% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perform..
Charpy Impact Unnotched 7.29 J/cm²

@Temperature -30.0 °C
34.7 ft-lb/in²

@Temperature -22.0 °F
Arkema Group Rilsan® BZM 43 G9 Nylon 11, 43% Glass Fiber Filled (Conditioned)
Designation ISO 1874-PA11,MS,18-080,(G+C)(F+D)(45+05)Rigid grade with glass fiber (43%) and graphite filler for injection molding. Available color: steel black gray. Additive free.High rigidity. Hig..
Charpy Impact Unnotched 7.30 J/cm²
34.7 ft-lb/in²
DAM; ISO 179/1eU
DuPont Performance Polymers Zytel® 80G14AHS NC010 Nylon 66  (Unverified Data**)
14% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G14AHS NC010 is a 14% glass fiber reinforced toughened high flow heat stabilized polyamide 66 resin. It offers outstanding perform..