Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 2.00 - 3.70 J/cm² @Temperature -30.0 - -30.0 °C |
9.52 - 17.6 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 2.97 J/cm² Grade Count:7 |
Overview of materials for Polycarbonate, Glass + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass + PTFE Filled". Each property range of values reported is minimum and maximum value.. |