Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 6.20 J/cm² | 29.5 ft-lb/in² | DIN 53453 |
Nilit FRIANYL B63 HS-GV 5 Nylon 6 for injection molding, 5% glass fiber reinforced Nylon 6 for injection molding, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 6.20 J/cm² | 29.5 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 1-7805 Polyamide 66, with glass fiber, aramid reinforcement and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Heat stabilised.High dimension.. |
|||
Charpy Impact Unnotched | 6.20 J/cm² @Temperature -20.0 °C |
29.5 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eU |
Borealis Daplen™ ED206HP TPO Compound Daplen ED206HP is a 25% mineral reinforced compound intended for injection molding. ED206HP has been developed especially for the car industry, to be used in interior parts requiring excellent scra.. |
|||
Charpy Impact Unnotched | 6.20 J/cm² @Temperature -20.0 °C |
29.5 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eU |
Borealis Xmod™ BE677AI High Crystalline Polypropylene Copolymer Xmod BE677AI is a UV-stabilized HCPP intended for injection molding of automotive interior and appliance parts. Xmod BE677AI has an excellent balance between impact strength and stiffness as well .. |
|||
Charpy Impact Unnotched | 6.20 J/cm² @Temperature 23.0 °C |
29.5 ft-lb/in² @Temperature 73.4 °F |
dry; ISO 179/1eU |
DSM Akulon® N24-G6 PA6-GF30 30% Glass Reinforced |
|||
Charpy Impact Unnotched | 6.20 J/cm² | 29.5 ft-lb/in² | ISO 179/IeU |
Addiplast Addinyl B2I V25 Flame Retardant Nylon 6, 25% Glass Filled Flame retardant, 25% glass fiber reinforced, halogen freeInformation provided by Addiplast. |
|||
Charpy Impact Unnotched | 6.20 J/cm² | 29.5 ft-lb/in² | Conditioned; ISO 179/IeU |
Addiplast Addinyl B2I V25 Flame Retardant Nylon 6, 25% Glass Filled Flame retardant, 25% glass fiber reinforced, halogen freeInformation provided by Addiplast. |