Mechanical Properties Metric English Comments
Charpy Impact Unnotched 2.00 - 2.50 J/cm²

@Temperature -30.0 - -30.0 °C
9.52 - 11.9 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 2.25 J/cm² Grade Count:2
Overview of materials for Polyaryletherketone (PAEK), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Carbon Fiber Filled". Each property range of values reported is minimum and ..
Charpy Impact Unnotched 1.30 - 2.50 J/cm²
6.19 - 11.9 ft-lb/in²
Average value: 1.65 J/cm² Grade Count:15
Overview of materials for Cyclo Olefin Polymer
This property data is a summary of similar materials in the MatWeb database for the category "Cyclo Olefin Polymer". Each property range of values reported is minimum and maximum values of appropria..
Charpy Impact Unnotched 0.400 - 2.50 J/cm²
1.90 - 11.9 ft-lb/in²
Average value: 1.38 J/cm² Grade Count:4
Overview of materials for Silicone, Molded, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Silicone, Molded, Glass Fiber Filled". Each property range of values reported is minimum and maximum val..
Charpy Impact Unnotched 1.00 - 2.50 J/cm²

@Temperature -30.0 - -20.0 °C
4.76 - 11.9 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 2.00 J/cm² Grade Count:4
Overview of materials for Nylon 6, 20% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are includ..
Charpy Impact Unnotched 2.50 - 2.50 J/cm²

@Temperature -20.0 - -20.0 °C
11.9 - 11.9 ft-lb/in²

@Temperature -4.00 - -4.00 °F
Average value: 2.50 J/cm² Grade Count:1
Overview of materials for Nylon 66, Mineral Filled, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Mineral Filled, Impact Grade". Each property range of values reported is minimum and maximum v..
Charpy Impact Unnotched 2.50 - 2.50 J/cm²

@Temperature -20.0 - -20.0 °C
11.9 - 11.9 ft-lb/in²

@Temperature -4.00 - -4.00 °F
Average value: 2.50 J/cm² Grade Count:2
Overview of materials for Polyphenylene Ether, 20% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 20% Glass Filled". Specific grades with glass content between 15% and 24% are inclu..
Charpy Impact Unnotched 2.00 - 2.50 J/cm²

@Temperature -20.0 - -20.0 °C
9.52 - 11.9 ft-lb/in²

@Temperature -4.00 - -4.00 °F
Average value: 2.25 J/cm² Grade Count:2
Overview of materials for Polyphenylene Ether, 30% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 30% Glass Filled". Specific grades with glass content between 25% and 34% are inclu..
Charpy Impact Unnotched 1.00 - 2.50 J/cm²
4.76 - 11.9 ft-lb/in²
Average value: 1.70 J/cm² Grade Count:4
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled". Each property range of values repo..
Charpy Impact Unnotched 1.50 - 2.50 J/cm²

@Temperature -30.0 - 5.00 °C
7.14 - 11.9 ft-lb/in²

@Temperature -22.0 - 41.0 °F
Average value: 2.00 J/cm² Grade Count:3
Overview of materials for Polyethylene Terephthalate (PET), 20% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 20% Glass Reinforced". Specific grades with glass content between 15% ..