Mechanical Properties Metric English Comments
Charpy Impact Unnotched 0.473 J/cm² - NB
2.25 ft-lb/in² - NB
Average value: 5.66 J/cm² Grade Count:158
Overview of materials for Polyphthalamide (PPA)
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide". Each property range of values reported is minimum and maximum values of appropriate Ma..