Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 1.70 - 4.00 J/cm² @Temperature -30.0 - -20.0 °C |
8.09 - 19.0 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 2.78 J/cm² Grade Count:4 |
Overview of materials for Polyphthalamide (PPA), 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are.. |
|||
Charpy Impact Unnotched | 1.00 - 4.00 J/cm² | 4.76 - 19.0 ft-lb/in² | Average value: 3.00 J/cm² Grade Count:38 |
Overview of materials for Polycarbonate, Carbon Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximum v.. |
|||
Charpy Impact Unnotched | 1.80 - 4.00 J/cm² @Temperature -30.0 - 30.0 °C |
8.57 - 19.0 ft-lb/in² @Temperature -22.0 - 86.0 °F |
Average value: 2.45 J/cm² Grade Count:4 |
Overview of materials for Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled". Specific grades with glass content between 35% an.. |
|||
Charpy Impact Unnotched | 4.00 - 4.00 J/cm² @Temperature -30.0 - -30.0 °C |
19.0 - 19.0 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 4.00 J/cm² Grade Count:2 |
Overview of materials for Liquid Crystal Polymer (LCP), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Mineral Filled". Each property range of values reported is minimum and max.. |
|||
Charpy Impact Unnotched | 1.20 - 4.00 J/cm² | 5.71 - 19.0 ft-lb/in² | Average value: 2.33 J/cm² Grade Count:3 |
Overview of materials for Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler". Specific grades with glass content between 45%.. |
|||
Charpy Impact Unnotched | 3.00 - 4.00 J/cm² @Temperature -30.0 - -20.0 °C |
14.3 - 19.0 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 3.50 J/cm² Grade Count:8 |
Overview of materials for Nylon 66, Carbon Fiber/PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Carbon Fiber/PTFE Filled". Each property range of values reported is minimum and maximum value.. |
|||
Charpy Impact Unnotched | 1.50 - 4.00 J/cm² | 7.14 - 19.0 ft-lb/in² | Average value: 2.75 J/cm² Grade Count:4 |
Overview of materials for Nylon 66, Stainless Steel Filled; EMI Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Stainless Steel Filled; EMI Grade". Each property range of values reported is minimum and maxi.. |
|||
Charpy Impact Unnotched | 3.00 - 4.00 J/cm² | 14.3 - 19.0 ft-lb/in² | ISO 179 |
Bulk Molding Compounds tetra-DUR N 4303 Bulk Molding Compound Mechanical high grade standard product.Typical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion p.. |
|||
Charpy Impact Unnotched | 3.50 - 4.00 J/cm² | 16.7 - 19.0 ft-lb/in² | Average value: 3.90 J/cm² Grade Count:5 |
Overview of materials for Polyphenylene Ether + Styrene-Butadiene Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether + Styrene-Butadiene Blend, Glass Filled". Each property range of values reported is .. |
|||
Charpy Impact Unnotched | 3.50 - 4.00 J/cm² @Temperature -30.0 - -30.0 °C |
16.7 - 19.0 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 3.90 J/cm² Grade Count:5 |
Overview of materials for Polyphenylene Ether + Styrene-Butadiene Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether + Styrene-Butadiene Blend, Glass Filled". Each property range of values reported is .. |
|||
Charpy Impact Unnotched | 1.30 - 4.00 J/cm² | 6.19 - 19.0 ft-lb/in² | Average value: 2.85 J/cm² Grade Count:13 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass + Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass + Mineral Filled". Each property range of values reported is min.. |
|||
Charpy Impact Unnotched | 2.10 - 4.00 J/cm² @Temperature -30.0 - 30.0 °C |
9.99 - 19.0 ft-lb/in² @Temperature -22.0 - 86.0 °F |
Average value: 2.90 J/cm² Grade Count:10 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass + Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass + Mineral Filled". Each property range of values reported is min.. |
|||
Charpy Impact Unnotched | 3.00 - 4.00 J/cm² | 14.3 - 19.0 ft-lb/in² | Average value: 3.72 J/cm² Grade Count:8 |
Overview of materials for Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant". Each property range of values re.. |
|||
Charpy Impact Unnotched | 2.00 - 4.00 J/cm² @Temperature -40.0 - -30.0 °C |
9.52 - 19.0 ft-lb/in² @Temperature -40.0 - -22.0 °F |
Average value: 3.07 J/cm² Grade Count:6 |
Overview of materials for Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant". Each property range of values re.. |
|||
Charpy Impact Unnotched | 4.00 - 4.00 J/cm² @Temperature -30.0 - -30.0 °C |
19.0 - 19.0 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 4.00 J/cm² Grade Count:1 |
Overview of materials for Polysulfone, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are inc.. |
|||
Charpy Impact Unnotched | 4.00 - 4.00 J/cm² @Temperature -30.0 - -30.0 °C |
19.0 - 19.0 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 4.00 J/cm² Grade Count:1 |
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Fiber Filled". Each property range of values reported is minimu.. |