Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 0.650 J/cm² @Temperature 23.0 °C |
3.09 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/2 eU |
Hexion Bakelite™ PF 51 Phenolic Formaldehyde Resin, Special Preparation Cylindrical Pellets
(discontinued **) Phenolic molding compound, organically filled, reinforced with cotton fibers, increased notched impact strength, standardized molding compound.Application areas: Contact support power switch, switch.. |
|||
Charpy Impact Unnotched | 0.650 J/cm² @Temperature 23.0 °C |
3.09 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/2 eU |
Hexion Bakelite™ PF 85 Phenolic Formaldehyde Resin, UL Listed
(discontinued **) Phenolic molding compound, organically filled, reinforced with cotton fibers, average notched impact strength, UL listed molding compound 1.5 mm/HB (BK, BN).Application areas: Switch covers, rolls, .. |
|||
Charpy Impact Unnotched | 0.650 J/cm² @Temperature 23.0 °C |
3.09 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/2 eU |
Hexion Bakelite™ 151733 Phenolic Formaldehyde Resin
(discontinued **) Phenolic molding compound, mainly organically filled, standard molding compound for normal stress.Application areas: Contact strips.Information provided by Bak AGBak AG became a part of Hexion in 20.. |
|||
Charpy Impact Unnotched | 0.650 J/cm² @Temperature 23.0 °C |
3.09 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/2 eU |
Hexion Bakelite™ 460124 Phenolic Formaldehyde Resin
(discontinued **) Phenolic molding compound, mainly organically filled, standard molding compound for normal stress.Application areas: Cookware fittings, electric devices.Information provided by Bak AGBak AG became a.. |
|||
Charpy Impact Unnotched | 0.650 J/cm² @Temperature 23.0 °C |
3.09 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/2 eU |
Hexion Bakelite™ X22 Phenolic Formaldehyde Resin, UL Listed
(discontinued **) Phenolic molding compound, mainly organically filled, UL listed molding compound 3.0 mm/V-0 (BN, BK).Application areas: Pot handles, operating controls, electrical isolators, housing parts.Informati.. |
|||
Charpy Impact Unnotched | 0.650 J/cm² @Temperature 23.0 °C |
3.09 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/2 eU |
Hexion Bakelite™ X24 Phenolic Formaldehyde Resin
(discontinued **) Phenolic molding compound, mainly organically filled.Application areas: Operating controls, housing parts, lamp holders.Information provided by Bak AGBak AG became a part of Hexion in 2005. |
|||
Charpy Impact Unnotched | 0.650 J/cm² @Temperature 23.0 °C |
3.09 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/2 eU |
Hexion Bakelite™ X30 Phenolic Formaldehyde Resin
(discontinued **) Phenolic molding compound, reinforced with cotton and sisal fibers, increased notched impact strength.Application areas: Covers for electrical and electromagnetic devices.Information provided by Bak.. |
|||
Charpy Impact Unnotched | 0.650 J/cm² @Temperature 23.0 °C |
3.09 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/2 eU |
Hexion Bakelite™ X65 Phenolic Formaldehyde Resin, UL Listed
(discontinued **) Phenolic molding compound, inorganically/organically filled, good heat-resistance and dimensional stability, UL listed molding compound 3.0 mm/V-0 (BN, BK).Application areas: Oven strips.Information.. |
|||
Charpy Impact Unnotched | 0.650 - 0.800 J/cm² | 3.09 - 3.81 ft-lb/in² | ISO 179 |
Vyncolit 2920 W Novolac Phenolic Mineral and organic filled molding compound with good dimensional stability and heat resistance.USES: Carburettor and intake manifold thermal insulator.Information provided by Vyncolit, a Sumitomo B.. |
|||
Charpy Impact Unnotched | 0.650 - 0.800 J/cm² @Temperature 23.0 °C |
3.09 - 3.81 ft-lb/in² @Temperature 73.4 °F |
Injection; ISO 179/ 1eU |
Raschig Group 5557 DAP
(discontinued **) Glass fiber-reinforced and inorganically filled diallylphthalate molding compound (DAP) in various colors. Good mechanical strength together with retention of high electrical properties under hot h.. |
|||
Charpy Impact Unnotched | 0.650 - 999.9 J/cm² @Temperature -40.0 - -20.0 °C |
3.09 - 4759 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 3.16 J/cm² Grade Count:26 |
Overview of materials for Polypropylene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Flame Retardant". Each property range of values reported is minimum and maximum values of.. |
|||
Charpy Impact Unnotched | 0.650 J/cm² @Temperature 23.0 °C |
3.09 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/2 eU |
Hexion Bakelite™ PF 8052 Phenolic Formaldehyde Resin, Resistant to High Temperatures
(discontinued **) Phenolic molding compound, glass fiber reinforced and inorganically filled. Excellent heat resistance with respect to surface finish and mechanical properties.Application areas: Pan handles, heat r.. |