Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 0.100 J/cm² @Temperature 23.0 °C |
0.476 ft-lb/in² @Temperature 73.4 °F |
ISO 179/2C |
SABIC Innovative Plastics Cycolac® INP572 ABS High molecular weight SAN, functions as a carrier resin for color concentrates. Can be used as compounding additives for polymer blends. Can be blended with high rubber graft modifier resins to pro.. |
|||
Charpy Impact Unnotched | 0.100 J/cm² | 0.476 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics Cycolac® INP572 ABS+SAN High molecular weight SAN, functions as a carrier resin for color concentrates. Can be used as compounding additives for polymer blends. Can be blended with high rubber graft modifier resins to pro.. |
|||
Charpy Impact Unnotched | 0.100 J/cm² @Temperature 23.0 °C |
0.476 ft-lb/in² @Temperature 73.4 °F |
ISO 179/2C |
SABIC Innovative Plastics Cycolac® INP576 ABS Can be used as compounding additives for polymer blends. Medium molecular weight SAN. Can be blended with high rubber graft modifier resins to produce customized ABS properties. Suitable for direc.. |
|||
Charpy Impact Unnotched | 0.100 J/cm² | 0.476 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics Cycolac® INP576 ABS+SAN Can be used as compounding additives for polymer blends. Medium molecular weight SAN. Can be blended with high rubber graft modifier resins to produce customized ABS properties. Suitable for direc.. |