Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Charpy Impact, Notched = 4.60 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 4.60 J/cm²

@Temperature 23.0 °C
21.9 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Nyco NYGLOS® 4W STO105 Wollastonite in Polypropylene
Data for polypropylene reinforced with 15% Nyco NYGLOS® 4W STO105 Wollastonite. Polypropylene used is Braskem TI6200Q High Impact Copolymer 20 MFR -NBWollastonite (calcium metasilicate, or CaSiO3)..
Charpy Impact, Notched 4.60 J/cm²

@Temperature 23.0 °C
21.9 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Arkema Group Pebax® Rnew 72R53 SP 01 Polyether Block Amide (PEBA)
Polyether block amide Pebax® 72R53 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide based on renewable resources. This SP grade has been developed to be heat and UV..
Charpy Impact, Notched 4.60 J/cm²

@Temperature 23.0 °C
21.9 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Borealis Daplen™ EF103AE Polypropylene TPO Compound
Daplen™ EF103AE is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties, high melt flow rate an..
Copyright © lookpolymers.com All Rights Reserved