Polymer Property : Charpy Impact, Notched = 3.80 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.798 J/cm²

@Temperature -30.0 °C
3.80 ft-lb/in²

@Temperature -22.0 °F
Complete Break; ISO 179
ExxonMobil Exxtral™ BMU 130 Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance for automotive exterior applications such as bumper fascia.Availability: Europe F..
Charpy Impact, Notched 0.798 J/cm²

@Temperature -20.0 °C
3.80 ft-lb/in²

@Temperature -4.00 °F
Complete Break; ISO 179
ExxonMobil Exxtral™ BMU 131 Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance, good surface appearance and good weatherability designed for automotive exterior ..
Charpy Impact, Notched 0.798 J/cm²

@Temperature -20.0 °C
3.80 ft-lb/in²

@Temperature -4.00 °F
Complete Break; ISO 179
ExxonMobil Exxtral™ BMU 139 Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance for automotive exterior applications such as bumper fascia.Availability: Asia Paci..
Charpy Impact, Notched 0.798 J/cm²

@Temperature 0.000 °C
3.80 ft-lb/in²

@Temperature 32.0 °F
Complete Break; ISO 179
ExxonMobil Exxtral™ BMU 143 Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance and designed for automotive interior application in which good surface finish, hig..
Charpy Impact, Notched 0.798 J/cm²

@Temperature 0.000 °C
3.80 ft-lb/in²

@Temperature 32.0 °F
Complete Break; ISO 179
ExxonMobil Exxtral™ BMU 143S Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance and designed for automotive interior application in which good surface finish, hig..
Charpy Impact, Notched 0.798 J/cm²

@Temperature -30.0 °C
3.80 ft-lb/in²

@Temperature -22.0 °F
Complete Break; ISO 179
ExxonMobil Exxtral™ H1725W Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin with very high flow. Product presenting very high rigidity, maintaining excellent impact resistance properties, including at a low tem..
Charpy Impact, Notched 0.798 J/cm²

@Temperature 0.000 °C
3.80 ft-lb/in²

@Temperature 32.0 °F
ISO 179/1eA
ExxonMobil PP4031E2 Polypropylene Impact Copolymer
Product Description: An impact copolymer resin for extrusion applications with high melt viscosity and excellent rigidity, shock resistance and dimensional stability. It is designed for corrugated ..
Charpy Impact, Notched 0.798 J/cm²

@Temperature 22.8 °C
3.80 ft-lb/in²

@Temperature 73.0 °F
ISO 179/1eA
ExxonMobil PP7075L1 Polypropylene Impact Copolymer
Product Description: A nucleated impact copolymer resin with high flow and antistatic properties. It is suitable for molding applications like disposable houseware, consumer products, toys and rigi..
Charpy Impact, Notched 0.798 J/cm²

@Temperature 22.8 °C
3.80 ft-lb/in²

@Temperature 73.0 °F
ISO 179/1eA
ExxonMobil PPU0009F Polypropylene Impact Copolymer
Product Description: An unstabilized impact copolymer resin designed for automotive and compounding applications.Availability: Europe Processing Method: CompoundingInformation provided by ExxonMobi..