Mechanical Properties Metric English Comments
Charpy Impact, Notched 2.70 J/cm²

@Temperature 23.0 °C
12.8 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Polykemi AB POLYfill PP CIP1001F Polypropylene
Information provided by Polykemi AB
Charpy Impact, Notched 2.70 J/cm²

@Temperature 23.0 °C
12.8 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Polykemi AB POLYfill PPC K5040 E30 Polypropylene Copolymer, Mineral Reinforced, Elastomer Modified
Information provided by Polykemi AB
Charpy Impact, Notched 2.70 J/cm²

@Temperature 23.0 °C
12.8 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
DSM Akulon® K224-HG5 (Cond.) 25% Glass Reinforced Nylon 6 (North America)  (discontinued **)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
Charpy Impact, Notched 2.70 J/cm²

@Temperature 23.0 °C
12.8 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
DSM Akulon® K224-HG5 Nylon 6-25% Glass Reinforced (European and Asian Grade) (Cond)  (discontinued **)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
Charpy Impact, Notched 2.70 J/cm²

@Temperature 23.0 °C
12.8 ft-lb/in²

@Temperature 73.4 °F
DAM; ISO 179/1eA
DuPont Performance Polymers Zytel® BM73G15THS BK317 Nylon 6  (Unverified Data**)
Zytel® BM73G15THS is a 15% glass fiber reinforced, heat stabilized, lubricated, toughened polyamide 6 for blow molding.Information provided by DuPont Performance Polymers
Charpy Impact, Notched 2.70 J/cm²

@Temperature 23.0 °C
12.8 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1A
Gromax BTE25-DN00N1 Nylon 6 (Dry)
Information provided by Gromax Enterprises Corp.
Charpy Impact, Notched 2.70 J/cm²

@Temperature 23.0 °C
12.8 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Solvay TECHNYL® eXten D238 V30 Nylon 6,10, 30% glass fiber, DRY
Description: TECHNYL® eXten D 238 V30 is a PA6,10 30% glass fiber reinforced and impact modified suitable for injection molding. TECHNYL® eXten D 238 V30 is based on a partially bio-sourced po..
Charpy Impact, Notched 2.70 J/cm²

@Temperature 23.0 °C
12.8 ft-lb/in²

@Temperature 73.4 °F
cond; ISO 179/1eA
DSM Novamid® 1013G45 1 NA PA6-GF45
45% Glass Reinforced, Injection Molding
Charpy Impact, Notched 2.70 J/cm²

@Temperature 23.0 °C
12.8 ft-lb/in²

@Temperature 73.4 °F
cond; ISO 179/1eA
DSM Novamid® 1013GH45 1 NA/BK701 PA6-GF45
45% Glass Reinforced, Heat Stabilized, Injection Molding
Charpy Impact, Notched 2.70 J/cm²

@Temperature 23.0 °C
12.8 ft-lb/in²

@Temperature 73.4 °F
DAM; ISO 179/1eA
DuPont Performance Polymers Zytel® EFE8089B BK416 Nylon 66
Zytel® EFE8089B BK416 is a 33% fiber reinforced, heat stabilized, lubricated, toughened polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Charpy Impact, Notched 2.70 J/cm²

@Temperature 23.0 °C
12.8 ft-lb/in²

@Temperature 73.4 °F
50%RH; ISO 179/1eA
DuPont Performance Polymers Zytel® 80G33HS1L BK104 Nylon 66  (Unverified Data**)
Zytel® 80G33HS1L BK104 is a 33% glass fiber reinforced, heat stabilized black polyamide 66 resin with outstanding impact resistance developed using DuPont Super Tough technology.Information provide..
Charpy Impact, Notched 2.70 J/cm²

@Temperature 23.0 °C
12.8 ft-lb/in²

@Temperature 73.4 °F
ISO 179
LG Chemical HF-380 ABS, High Flow, High Impact
Feature: Injection Molding, High FlowApplication: Electric & Electronic Products, Toys, Miscellaneous Goods)CAS No. 9003-56-9Information Provided by LG Chem