Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 2.52 J/cm² @Temperature 22.8 °C |
12.0 ft-lb/in² @Temperature 73.0 °F |
Partial Break; ISO 179 |
ExxonMobil Exxtral™ BNT 013 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin designed for injection molded automotive interior applications such as door panels.Availability: Africa & Middle East, Asia Pacific, E.. |
|||
Charpy Impact, Notched | 2.52 J/cm² @Temperature 22.8 °C |
12.0 ft-lb/in² @Temperature 73.0 °F |
Partial Break; ISO 179 |
ExxonMobil Exxtral™ CNK 010 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin designed for injection or extrusion automotive applications with low melt and excellent low temperature impact. Availability: Africa &.. |