Polymer Property : Charpy Impact, Notched = 2.05 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.430 J/cm²

@Temperature -30.0 °C
2.05 ft-lb/in²

@Temperature -22.0 °F
Radici Radilon® A ECP3808 (cond.) Nylon 66
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov..
Charpy Impact, Notched 0.430 J/cm²

@Temperature -30.0 °C
2.05 ft-lb/in²

@Temperature -22.0 °F
Radici Radilon® S RCV3015 (cond.) Nylon 6
Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group.
Charpy Impact, Notched 0.430 J/cm²

@Temperature 23.0 °C
2.05 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Polyram PlusTek PB340S50 Nylon 6 for Injection Molding, 50% Glass-beads Reinforced, Heat Stabilized
50% Glass-beads reinforced, heat stabilized Nylon 6 for injection molding applications.Information provided by Polyram.
Charpy Impact, Notched 0.430 J/cm²

@Temperature 23.0 °C
2.05 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
DSM Akulon® S223-GM35 (Dry) 15% Glass Reinforced, 25% Mineral Reinforced Nylon 66 (North America)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
Charpy Impact, Notched 0.430 J/cm²

@Temperature -30.0 °C
2.05 ft-lb/in²

@Temperature -22.0 °F
Radici Radilon® S LHS (dry) Nylon 6
Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group.