Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 11.7 J/cm² @Temperature 23.0 °C |
55.7 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Solvay TECHNYL® eXten D 458P PA6.10, Conditioned Description: Product in development - provisional datasheet. High viscosity unfilled plasticized PA6.10 for extrusion applications providing low end part warpage.Available in: Asia Pacific, Europe, .. |