Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Charpy Impact, Notched = 10.9 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 2.30 J/cm²

@Thickness 102 mm,
Temperature 23.0 °C
10.9 ft-lb/in²

@Thickness 4.00 in,
Temperature 73.4 °F
ISO 179
Premix Thermoplastics PRE-ELEC® PE 1200 Conductive Thermoplastic Compound
PRE-ELEC® PE 1200 is a conductive thermoplastic masterbatch/compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. PRE-ELEC® PE 1200 has a high concentration o..
Charpy Impact, Notched 2.30 J/cm²

@Temperature 23.0 °C
10.9 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Polykemi AB POLYelast TPE HJ752 Thermoplastic Elastomer, PP/Elastomer, Mineral Reinforced
Information provided by Polykemi AB
Charpy Impact, Notched 2.30 J/cm²

@Temperature 23.0 °C
10.9 ft-lb/in²

@Temperature 73.4 °F
Radici Radilon® S LHS (cond.) Nylon 6
Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group.
Charpy Impact, Notched 2.30 J/cm²

@Temperature 23.0 °C
10.9 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Polykemi AB POLYfill PP HJ752 Polypropylene/Elastomer, Mineral Reinforced
Information provided by Polykemi AB
Charpy Impact, Notched 2.30 J/cm²

@Temperature 23.0 °C
10.9 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Polykemi AB POLYfill PP HJ752 UV Polypropylene/Elastomer, Mineral Reinforced
Information provided by Polykemi AB
Charpy Impact, Notched 2.30 J/cm²

@Temperature 23.0 °C
10.9 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
DuPont Performance Polymers Delrin® 100T BK602 Acetal Homopolymer  (Unverified Data**)
Delrin® 100T BK602 is a toughened, high viscosity acetal homopolymer grade with superior impact resistance. It is designed for highly stressed parts where outstanding toughness is required.Informa..
Charpy Impact, Notched 2.30 J/cm²

@Temperature 23.0 °C
10.9 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
DSM Akulon® Ultraflow™ K-FHG7 Nylon 6-35% Glass Reinforced (European Grade) (Cond)  (discontinued **)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
Charpy Impact, Notched 2.30 J/cm²

@Temperature 23.0 °C
10.9 ft-lb/in²

@Temperature 73.4 °F
50%RH; ISO 179/1eA
DuPont Performance Polymers Zytel® 73G30HSL BK416 Nylon 6  (Unverified Data**)
Zytel® 73G30HSL BK416 is a 30% glass fiber reinforced, heat stabilized, lubricated, black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
Charpy Impact, Notched 2.30 J/cm²

@Temperature 23.0 °C
10.9 ft-lb/in²

@Temperature 73.4 °F
50%RH; ISO 179/1eA
DuPont Performance Polymers Zytel® 73G30HSL NC010 Nylon 6  (Unverified Data**)
Zytel® 73G30HSL NC010 is a 30% glass fiber reinforced, heat stabilized polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
Charpy Impact, Notched 2.30 J/cm²

@Temperature -20.0 °C
10.9 ft-lb/in²

@Temperature -4.00 °F
50%RH; ISO 179/1eA
DuPont Performance Polymers Zytel® ST7301 NC010 Nylon 6  (Unverified Data**)
Zytel® ST7301 NC010 is a Super Tough, heat stabilized, lubricated polyamide 6 resin for injection molding and extrusion. It offers outstanding impact resistance over a wide temperature and humidity..
Charpy Impact, Notched 2.30 J/cm²

@Temperature 23.0 °C
10.9 ft-lb/in²

@Temperature 73.4 °F
ISO 179
LG Chemical EF-378 ABS, Flame Retardant, Halogen Free
Information Provided by LG Chem
Charpy Impact, Notched 2.30 J/cm²

@Temperature 23.0 °C
10.9 ft-lb/in²

@Temperature 73.4 °F
ISO 179
LG Chemical HI-151 ABS, Middle Impact
Information Provided by LG Chem
Charpy Impact, Notched 2.30 J/cm²

@Temperature 23.0 °C
10.9 ft-lb/in²

@Temperature 73.4 °F
ISO 179
LG Chemical XR-472 ABS, High Heat Resistance, High Gloss
Information Provided by LG Chem
Charpy Impact, Notched 2.30 J/cm²

@Temperature 23.0 °C
10.9 ft-lb/in²

@Temperature 73.4 °F
Conditioned; ISO 179/1eA
Lanxess Durethan® AKV 50 H2.0 901510 Nylon 66, 50% Glass Fiber
PA 66, injection molding grade, 50% glass fibers, good heat-ageing resistance
Charpy Impact, Notched 2.30 J/cm²

@Temperature 23.0 °C
10.9 ft-lb/in²

@Temperature 73.4 °F
cond.; ISO 179-1eA
Lanxess Durethan® AKV 40 H2.0 901510 Nylon 66, Glass Fiber Reinforced
PA 66, 40% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS.
Charpy Impact, Notched 2.30 J/cm²

@Temperature 23.0 °C
10.9 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Solvay TECHNYL® C 246SI V30 PA6, 30% glass filled, DRY
Description: Polyamide 6, reinforced with 30 % of glass fiber, with high impact resistance, for injection molding.Available in: Asia Pacific , Europe and North AmericaProduct Applications: Having go..
Charpy Impact, Notched 2.30 J/cm²

@Temperature 23.0 °C
10.9 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Suzhou Hipro Polymers Hiprolon® 400 MC HLS G30 Nylon, 30% glass fiber filled
Hiprolon® 400 MC HLS G30 is a specialty long chain polyamide compound reinforced with 30% chopped glass fiber for injection molding. It contains some bio-renewable resources Features: high dime..
Charpy Impact, Notched 2.30 J/cm²

@Temperature 23.0 °C
10.9 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Sax Polymers SAXATEC 4307 Acrylonitrile Styrene Acrylate
SAXATEC 4307 is a high impact resistant, high viscosity and weatherable ASA injection molding grade, characterized by high mechanical strength and good processabilityInformation provided by SAX Poly..
Charpy Impact, Notched 2.30 J/cm²

@Temperature 23.0 °C
10.9 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Polyram Polytron P40N03 Polypropylene, 40% Long Glass Fibers
Is a chemically coupled 40% long glass fibers reinforced natural polypropylene, heat stabilized, for injection molding applications. These products have significantly improved impact performance ch..
Charpy Impact, Notched 2.30 J/cm²

@Temperature 23.0 °C
10.9 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Unipetrol PP MONSTEN® MT 802 Polypropylene Random Copolymer
Applications include injection molding and extrusion. Antistatic and transparent stabilization. Random copolymer.Information provided by Unipetrol RPA
Charpy Impact, Notched 2.30 J/cm²

@Temperature 23.0 °C
10.9 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
DSM Arnitel® PL650 Injection Grade Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Charpy Impact, Notched 2.30 J/cm²

@Temperature 23.0 °C
10.9 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
DSM Arnitel® PL650 Polyether Ester Elastomer (European and Asian Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Charpy Impact, Notched 2.30 J/cm²

@Temperature -30.0 °C
10.9 ft-lb/in²

@Temperature -22.0 °F
DAM; ISO 179/1eA
DuPont Performance Polymers Zytel® BM7300THS BK317 Nylon 6  (Unverified Data**)
Zytel® BM7300THS is an unreinforced, heat stabilized, lubricated, toughened polyamide 6 for blow molding.Information provided by DuPont Performance Polymers
Charpy Impact, Notched 2.30 J/cm²

@Temperature -30.0 °C
10.9 ft-lb/in²

@Temperature -22.0 °F
DAM; ISO 179/1eA
DuPont Performance Polymers Zytel® ST801AW NC010 Nylon 66  (Unverified Data**)
Zytel® ST801AW NC010 is a Super Tough, high performance polyamide 66 resin. It is UV stabilized and when appropriately colored offers the best resistance to indirect sunlight in automotive interior..
Charpy Impact, Notched 2.30 J/cm²

@Temperature 23.0 °C
10.9 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Ascend Performance Materials Vydyne® 21SPF Nylon 66, General Purpose, High Productivity, Conditioned
Vydyne® 21SPF is general-purpose PA66 resin. Available in natural, it is designed principally for injection-molding fabrication. This grade offers a well-balanced combination of engineering propert..
Charpy Impact, Notched 2.30 J/cm²

@Temperature 23.0 °C
10.9 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Ascend Performance Materials Vydyne® 21SPF BLK Nylon 66, DAM
Vydyne® 21SPF BLK is a, general-purpose PA66 resin used for extrusion-compounding. Available in black, it is designed principally for injection-molding fabrication. This grade offers a well-balance..
Charpy Impact, Notched 2.30 J/cm²

@Temperature 23.0 °C
10.9 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Ascend Performance Materials Vydyne® 66B Nylon 66, General Purpose, high viscosity, Conditioned
Vydyne® 66B is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66B resin offers high strength, ..
Charpy Impact, Notched 2.30 J/cm²

@Temperature 23.0 °C
10.9 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Ascend Performance Materials Vydyne® 21SPF1 Nylon 66, Conditioned
Vydyne® 21SPF1 is a general-purpose PA66 resin available in natural color. It is designed principally for injection-molding applications with the added benefits of improved flow during the molding ..
Copyright © lookpolymers.com All Rights Reserved