Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 1.65 J/cm² @Temperature 23.0 °C |
7.85 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB SCANAMID 66 AL220L2M Nylon 66, Impact Modified Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 1.65 J/cm² @Temperature 23.0 °C |
7.85 ft-lb/in² @Temperature 73.4 °F |
50%RH; ISO 179/1eA |
DuPont Performance Polymers Zytel® RS 30G30L NC010 Nylon 610
(Unverified Data**) Zytel® RS 30G30L NC010 is a lubricated, 30% glass fiber reinforced polyamide 610 resin containing a minimum of 40% renewably sourced ingredients by weight (60% based on polymer only). It was initia.. |
|||
Charpy Impact, Notched | 1.65 J/cm² @Temperature 23.0 °C |
7.85 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® RS 30G30L NC010 Nylon 610
(Unverified Data**) Zytel® RS 30G30L NC010 is a lubricated, 30% glass fiber reinforced polyamide 610 resin containing a minimum of 40% renewably sourced ingredients by weight (60% based on polymer only). It was initia.. |