Mechanical Properties Metric English Comments
Charpy Impact, Notched 1.49 J/cm²

@Temperature 0.000 °C
7.10 ft-lb/in²

@Temperature 32.0 °F
Partial Break; ISO 179
ExxonMobil Exxtral™ BMT222 Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin characterized by good stiffness/toughness balance and designed for automotive interior applications in which good surface finish and g..
Charpy Impact, Notched 1.49 J/cm²

@Temperature 22.8 °C
7.10 ft-lb/in²

@Temperature 73.0 °F
ISO 179
ExxonMobil Exxtral™ BMU 141 Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance and designed for automotive instrument panels in which good surface finish, high s..
Charpy Impact, Notched 1.49 J/cm²

@Temperature 22.8 °C
7.10 ft-lb/in²

@Temperature 73.0 °F
Complete Break; ISO 179
ExxonMobil Exxtral™ BMU 143 Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance and designed for automotive interior application in which good surface finish, hig..
Charpy Impact, Notched 1.49 J/cm²

@Temperature 22.8 °C
7.10 ft-lb/in²

@Temperature 73.0 °F
Complete Break; ISO 179
ExxonMobil Exxtral™ BMU 143S Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance and designed for automotive interior application in which good surface finish, hig..
Charpy Impact, Notched 1.49 J/cm²

@Temperature 0.000 °C
7.10 ft-lb/in²

@Temperature 32.0 °F
Partial Break; ISO 179
ExxonMobil Exxtral™ BNT 010 Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin designed for automotive exterior painted parts such as bumper fascia.Availability: Africa & Middle East, Asia Pacific, Europe, South A..
Charpy Impact, Notched 1.49 J/cm²

@Temperature 0.000 °C
7.10 ft-lb/in²

@Temperature 32.0 °F
Complete Break; ISO 179
ExxonMobil Exxtral™ BNT 011 Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin with good UV resistance designed for automotive exterior parts such as bumper fascia.Availability: Africa & Middle East, Asia Pacific,..