Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.294 J/cm² @Temperature -30.0 °C |
1.40 ft-lb/in² @Temperature -22.0 °F |
Complete Break; ISO 179 |
ExxonMobil Exxtral™ BMV 301 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance, designed for automotive interior application in which good surface finish, high s.. |
|||
Charpy Impact, Notched | 0.294 J/cm² @Temperature -20.0 °C |
1.40 ft-lb/in² @Temperature -4.00 °F |
Complete Break; ISO 179 |
ExxonMobil Exxtral™ CMU 201 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin designed for automotive interior covered applications such as retainers in which a good stiffness toughness balance is required.Availa.. |
|||
Charpy Impact, Notched | 0.294 J/cm² @Temperature 0.000 °C |
1.40 ft-lb/in² @Temperature 32.0 °F |
Complete Break; ISO 179 |
ExxonMobil Exxtral™ CMW 203 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin characterized by high flow and designed for automotive interior applications such as door panel linings and other low pressure back mo.. |
|||
Charpy Impact, Notched | 0.294 J/cm² @Temperature -20.0 °C |
1.40 ft-lb/in² @Temperature -4.00 °F |
Complete Break; ISO 179 |
ExxonMobil Exxtral™ CNK 010 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin designed for injection or extrusion automotive applications with low melt and excellent low temperature impact. Availability: Africa &.. |
|||
Charpy Impact, Notched | 0.294 J/cm² @Temperature -20.0 °C |
1.40 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
ExxonMobil PPU0009F Polypropylene Impact Copolymer Product Description: An unstabilized impact copolymer resin designed for automotive and compounding applications.Availability: Europe Processing Method: CompoundingInformation provided by ExxonMobi.. |