Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.450 J/cm² @Temperature -30.0 °C |
2.14 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Nyco NYGLOS® 4W STO105 Wollastonite in Polypropylene Data for polypropylene reinforced with 15% Nyco NYGLOS® 4W STO105 Wollastonite. Polypropylene used is Braskem TI6200Q High Impact Copolymer 20 MFR -NBWollastonite (calcium metasilicate, or CaSiO3).. |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature 23.0 °C |
2.14 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB SCANCOMP PP BN140 T5 Polypropylene Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature -30.0 °C |
2.14 ft-lb/in² @Temperature -22.0 °F |
|
Radici Radilon® S 32HS (cond.) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature -30.0 °C |
2.14 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DuPont Performance Polymers Crastin® 6130 NC010 PBT
(Unverified Data**) Crastin® 6130 NC010 is an unreinforced, medium high viscosity polybutylene terephthalate resin for extrusion and injection molding.Information provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature -20.0 °C |
2.14 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYfill PPC 200 E20 Polypropylene Copolymer, Elastomer Modified Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature -20.0 °C |
2.14 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYfill PPH GF5020 PD1 VT2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled, Heat Stabilized Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature 23.0 °C |
2.14 ft-lb/in² @Temperature 73.4 °F |
|
Radici Radilon® A CP300K (cond.) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature -30.0 °C |
2.14 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DSM Akulon® Ultraflow™ K-FHGM44 Nylon 6-40% Glass and Mineral Reinforced (European and Asian Grade) (Cond)
(d The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature 23.0 °C |
2.14 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Inno-Comp INNOPOL® CS 2-2120 20% Talc-Filled Polypropylene Block-Copolymer INNOPOL® CS 2-2120 is a 20% talc-filled compound based on polypropylene block-copolymer. This grade is available in nature and custom colored form.INNOPOL® CS 2-2120 is developed for producing.. |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature 23.0 °C |
2.14 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Inno-Comp INNOPOL® CS 2-3130 NU UV-Stabilized 30% Talc-Filled Polypropylene Block-Copolymer INNOPOL® CS 2-3130 NU is an UV-stabilized 30% talc-filled polypropylene block-copolymer compound /PP-B TD30 (ISO 1043)/.INNOPOL® CS 2-3130 NU is recommended for producing injection molded prod.. |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature -30.0 °C |
2.14 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Inno-Comp INNOPOL® CS 2-9000 MA B Polypropylene Copolymer INNOPOL® CS 2-9000 MA B is a black colored, high melt flow copolymer with antistatic additive.INNOPOL® CS 2-9000 MA B is developed for producing injection molded automotive components.All info.. |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature 23.0 °C |
2.14 ft-lb/in² @Temperature 73.4 °F |
|
LATI Lastilac RT K/10 ABS, 10% Carbon Fiber Reinforced Acrylonitrile-Butadiene-Styrene copolymer (ABS) based compound. Carbon fiber. High dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInforma.. |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature -20.0 °C |
2.14 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
Borealis BA390TF Polypropylene Copolymer BA390TF is a high molecular weight, low melt flow rate polypropylene block copolymer with very high impact strength. Applications: BA390TF is recommended for foam extrusion, or thermoforming.Inform.. |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature -20.0 °C |
2.14 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
Borealis BD950MO Polypropylene Copolymer BD950MO is a heterophasic copolymer. This grade is intended for compression and injection molding. The main features of this grade are good stiffness and impact resistance, very good process ability.. |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature 23.0 °C |
2.14 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Borealis BJ356MO Polypropylene Copolymer BJ356MO is a heterophasic copolymer. This grade provides very high melt flow rate, very high stiffness and medium impact strength. and is designed for high-speed injection molding and contains nucle.. |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature -30.0 °C |
2.14 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Borealis Daplen™ ED117AE Polypropylene TPO Compound Daplen™ ED117AE is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and gives a good surfac.. |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature -30.0 °C |
2.14 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Borealis Daplen™ EH104AE Polypropylene TPO Compound Daplen™ EH104AE is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, high.. |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature 23.0 °C |
2.14 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Unipetrol PP MONSTEN® MT 825 Polypropylene Random Copolymer Made for injection molding applications. Antistatic and transparent stabilization. Random copolymer.Information provided by Unipetrol RPA |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature 23.0 °C |
2.14 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Unipetrol PP MONSTEN® MT 950 Polypropylene Random Copolymer Made for injection molding applications. Antistatic and transparent stabilization. Random copolymer.Information provided by Unipetrol RPA |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature -20.0 °C |
2.14 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Total PPC 10642 Polypropylene, Heterophasic Copolymer, Injection Molding Polypropylene PPC 10642 is a nucleated antistatic heterophasic copolymer with high Melt Flow index of 44 g/10 min.Polypropylene PPC 10642 is characterized by high fluidity with good mechanical prope.. |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature -20.0 °C |
2.14 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Total PPC 12642 Polypropylene, Heterophasic Copolymer, Injection Molding Polypropylene PPC 12642 is a nucleated antistatic heterophasic copolymer with high Melt Flow index of 70 g/10 min and good mechanical properties.Polypropylene PPC 10641 has been developed for high s.. |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature -20.0 °C |
2.14 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
Borealis Daplen™ EE188AI Polypropylene TPO Compound Daplen™ EE188AI is a 15% mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and is easy to process. .. |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature -20.0 °C |
2.14 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Total PPC 11750 Polypropylene, Heterophasic Copolymer, Injection Molding Polypropylene PPC 11750 is a nucleated and controlled-rheology heterophasic copolymer with very high Melt Flow index of 50 g/10 min.Polypropylene PPC 11750 is characterized by good impact resistance.. |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature -20.0 °C |
2.14 ft-lb/in² @Temperature -4.00 °F |
DIN 53453 |
Total PPC 4820WZ Polypropylene, Impact Copolymer TOTAL Petrochemicals Polypropylene 4820WZ is a nucleated impact copolymer with a Melt Flow index of 35 g/10 min.TOTAL Polypropylene 4820WZ is characterized by improved stiffness, creep resistance, h.. |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature -30.0 °C |
2.14 ft-lb/in² @Temperature -22.0 °F |
cond; ISO 179/1eA |
DSM Stanyl® TW241B3 PA46-CF15 15% Carbon Reinforced, Heat Stabilized, Lubricated |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature 23.0 °C |
2.14 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB POLYfill PPHC T11030 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature 23.0 °C |
2.14 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB POLYfill PPHC T8020 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature -30.0 °C |
2.14 ft-lb/in² @Temperature -22.0 °F |
|
Radici Radilon® A 35E 990 (dry) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature -30.0 °C |
2.14 ft-lb/in² @Temperature -22.0 °F |
|
Radici Radilon® A HSK (dry) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Charpy Impact, Notched | 0.450 J/cm² @Temperature 23.0 °C |
2.14 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Borealis MB350WG Polypropylene Compound, Mineral Filled MB350WG is a 30% mineral filled polypropylene compound intended for injection molding. This material has a very high impact strength while maintaining good stiffness and is easy to process. Applic.. |