Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.220 J/cm² @Temperature -20.0 °C |
1.05 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVAMID 6 GB 30 PA6, 30% glass beads FeaturesNearly ideal anisotropy of shrinkage in the vertical and in the horizontal direction is established. Manufacturing of exact mouldings. Disadvantage are the relatively low mechanical properti.. |
|||
Charpy Impact, Notched | 0.220 J/cm² @Temperature -20.0 °C |
1.05 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVAMID 6 GB 30 TS PA6, 30% glass beads FeaturesNearly ideal anisotropy of shrinkage in the vertical and in the horizontal direction is established. Manufacturing of exact mouldings. Disadvantage are the relatively low mechanical properti.. |
|||
Charpy Impact, Notched | 0.220 J/cm² @Temperature -30.0 °C |
1.05 ft-lb/in² @Temperature -22.0 °F |
|
Radici Radiflam® S FR (cond.) Nylon 6 PA6 flame retardant injection molding grade. Halogen and phosphorus free. Natural color. Suitable for monofilament extrusion.Information provided by Radici group. |
|||
Charpy Impact, Notched | 0.220 J/cm² @Temperature 23.0 °C |
1.05 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Inno-Comp INNOPOL® CS 1-2140 BLH 40% Talc-Filled Polypropylene Homopolymer INNOPOL® CS 1-2140 BLH is recommended especially for producing products, where high stiffness, low shrinkage, long term heat stability and excellent processability are required.All information pr.. |
|||
Charpy Impact, Notched | 0.220 J/cm² @Temperature -20.0 °C |
1.05 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
Inno-Comp INNOPOL® CS 3-9120 SR5 17% Talc Filled Polypropylene Blend INNOPOL® CS 3-9120 SR5 is a 17% talc-filled compound based on blend of polypropylene block copolymer and homopolymer. This grade is available in natural and custom colored form.INNOPOL® CS 3-9.. |
|||
Charpy Impact, Notched | 0.220 J/cm² @Temperature -30.0 °C |
1.05 ft-lb/in² @Temperature -22.0 °F |
|
Radici Radiflam® A AE (cond.) Nylon 66 Radiflam® A is a range of flame retardant polyamides 66 (PA 66) used for injection molding and extrusion for all applications where high fire resistance is required.Information provided by Radici g.. |