Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.0300 J/cm² @Temperature -20.0 °C |
0.143 ft-lb/in² @Temperature -4.00 °F |
|
LATI Latene® 7 TR-V2 PP Homopolymer, Mineral Reinforced, Flame Retardant Polypropylene homopolymer (PPh) based compound. Mineral filler. UL94 V-2 classified, with brominated flame retardants, PBB/PBDE free. Good surface appearance.Availability: Africa & Middle East; Asia.. |
|||
Charpy Impact, Notched | 0.0300 J/cm² @Temperature -20.0 °C |
0.143 ft-lb/in² @Temperature -4.00 °F |
|