Polymer Property : Izod Impact, Notched = 9.88 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 9.88 J/cm
18.5 ft-lb/in
NB; ASTM D256
LyondellBasell SEQUEL® E3000 TPO
Description: SEQUEL® E3000 thermoplastic olefinic elastomer (TPO) is designed for thermoformed exterior and interior applications that require toughness and dimensional stability. This extrusion..
Izod Impact, Notched 9.88 J/cm
18.5 ft-lb/in
Lengthwise; ASTM D256
Bedford Plastics Glass Reinforced FR Polyester Flat Sheet, 1/8"
Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod..
Izod Impact, Notched 9.88 J/cm
18.5 ft-lb/in
Lengthwise; ASTM D256
Bedford Plastics Glass Reinforced Vinylester Flat Sheet, 1/8"
Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod..
Izod Impact, Notched 9.88 J/cm
18.5 ft-lb/in
Lengthwise; ASTM D256
Bedford Plastics Glass Reinforced Polyester Flat Sheet 1/8"
Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded products feature:High StrengthCorrosion Resistant to many che..