Polymer Property : Izod Impact, Notched = 8.90 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 4.75 J/cm
8.90 ft-lb/in
ASTM D256
SABIC Innovative Plastics Cycoloy® CY6110 PC+ABS
Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la..
Izod Impact, Notched 4.75 J/cm
8.90 ft-lb/in
ASTM D256
SABIC Innovative Plastics Cycoloy® CY6110 PC+ABS (Asia Pacific)
Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la..
Izod Impact, Notched 4.75 J/cm
8.90 ft-lb/in
ASTM D256
SABIC HP7022 Low Density Polyethylene for Injection Molding
Product Description: HP7022 is a Low Density Polyethylene offering a unique combination of consistent processability, flexibility and toughness. Articles manufactured from HP7022 exhibit excellent..
Izod Impact, Notched 4.75 J/cm
8.90 ft-lb/in
ASTM D256
SABIC Innovative Plastics Cycoloy® CY6110 PC+ABS (Europe-Africa-Middle East)
Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la..
Izod Impact, Notched 4.75 J/cm
8.90 ft-lb/in
ASTM D-256
Glastic 1120 Corrosion-Resistant Panels
Glastic® Corrosion-Resistant Panels are ideal for applications where resistance to both flame, and the splash or spill of laboratory chemicals is important. Glastic® Grade 1120 is an asbestos..
Izod Impact, Notched 4.75 J/cm

@Thickness 3.20 mm
8.90 ft-lb/in

@Thickness 0.126 in
ASTM D256
SABIC Innovative Plastics ULTEM 2210R PEI
20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.
Izod Impact, Notched 4.75 J/cm

@Thickness 3.20 mm
8.90 ft-lb/in

@Thickness 0.126 in
ASTM D256
SABIC Innovative Plastics ULTEM 2210R PEI (Asia Pacific)
20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.
Izod Impact, Notched 4.75 J/cm
8.90 ft-lb/in
ASTM D256
ExxonMobil LLDPE LL 5002.09 Linear Low Density Polyethylene Resin
Product Description: LL 5002.09 is a linear low density polyethylene resin designed to provide good processability and ease of blending. LL 5002.09 also exhibits good toughness and environmental str..