Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 8.90 J/cm | 16.7 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® EXL1413T PC Copolymer Lexan* EXL1413T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers excellent low temperature (-30 °C) ductility in combination with medium f.. |
|||
Izod Impact, Notched | 8.90 J/cm | 16.7 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® EXL1413T PC Copolymer (Asia Pacific) Lexan* EXL1413T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers excellent low temperature (-30 °C) ductility in combination with medium f.. |
|||
Izod Impact, Notched | 8.90 J/cm | 16.7 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® EXL1433T PC Copolymer (Asia Pacific) Lexan* EXL1433T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding grade. This resin offers excellent low temperature (-30 C) ductility in combination with .. |
|||
Izod Impact, Notched | 8.90 J/cm | 16.7 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® EXL1433T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1433T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding grade. This resin offers excellent low temperature (-30 C) ductility in combination with .. |
|||
Izod Impact, Notched | 8.90 J/cm | 16.7 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® EXL1443T PC Copolymer Lexan* EXL1443T polycarbonate (PC) siloxane copolymer resin is an injection molding grade with FDA and EU food contact compliance. This resin offers excellent low temperature (-30 C) ductility in co.. |
|||
Izod Impact, Notched | 8.90 J/cm | 16.7 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® EXL1443T PC Copolymer (Asia Pacific) Lexan* EXL1443T polycarbonate (PC) siloxane copolymer resin is an injection molding grade with FDA and EU food contact compliance. This resin offers excellent low temperature (-30 C) ductility in co.. |
|||
Izod Impact, Notched | 8.90 J/cm | 16.7 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® EXL1443T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1443T polycarbonate (PC) siloxane copolymer resin is an injection molding grade with FDA and EU food contact compliance. This resin offers excellent low temperature (-30 C) ductility in co.. |
|||
Izod Impact, Notched | 8.90 J/cm | 16.7 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® EXL1463T PC Copolymer Lexan* EXL1463T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers excellent low temperature (-30 C) ductility in combination with medium flow ch.. |
|||
Izod Impact, Notched | 8.90 J/cm | 16.7 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® EXL1463T PC Copolymer (Asia Pacific) Lexan* EXL1463T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers excellent low temperature (-30 C) ductility in combination with medium flow ch.. |
|||
Izod Impact, Notched | 8.90 J/cm | 16.7 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® HPX4 PC Copolymer Medium flow specialty polycarbonate - improved processability & autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP.. |
|||
Izod Impact, Notched | 8.90 J/cm | 16.7 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® HPX4 PC Copolymer (Asia Pacific) Medium flow specialty polycarbonate - improved processability & autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP.. |
|||
Izod Impact, Notched | 8.90 J/cm | 16.7 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® HPX4EU PC Copolymer (Europe-Africa-Middle East) Medium flow specialty polycarbonate - improved processability & autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP.. |
|||
Izod Impact, Notched | 8.90 J/cm | 16.7 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® HPX4R PC Copolymer Medium flow specialty polycarbonate with outstanding processability, ductility and autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatib.. |
|||
Izod Impact, Notched | 8.90 J/cm | 16.7 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® HPX4R PC Copolymer (Asia Pacific) Medium flow specialty polycarbonate with outstanding processability, ductility and autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatib.. |
|||
Izod Impact, Notched | 8.90 J/cm | 16.7 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® HPX4REU PC Copolymer (Europe-Africa-Middle East) Medium flow specialty polycarbonate - improved processability & autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP.. |
|||
Izod Impact, Notched | 8.90 J/cm | 16.7 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® SD1278 PC Copolymer Lexan* SD1278 polycarbonate (PC) siloxane copolymer resin is a transparent extrusion grade for food contact applications for sheet extrusion. This resin offers extreme low temperature (-40 °C) .. |
|||
Izod Impact, Notched | 8.90 J/cm | 16.7 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® SD1278 PC Copolymer (Asia Pacific) Lexan* SD1278 polycarbonate (PC) siloxane copolymer resin is a transparent extrusion grade for food contact applications for sheet extrusion. This resin offers extreme low temperature (-40 °C) .. |
|||
Izod Impact, Notched | 8.90 J/cm | 16.7 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® SD1278 PC Copolymer (Europe-Africa-Middle East) Lexan* SD1278 polycarbonate (PC) siloxane copolymer resin is a transparent extrusion grade for food contact applications for sheet extrusion. This resin offers extreme low temperature (-40 °C) .. |
|||
Izod Impact, Notched | 8.90 J/cm | 16.7 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® FXD1413T PC Copolymer Clear PC-siloxane copolymer with excellent processability, in special light diffusion colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may af.. |
|||
Izod Impact, Notched | 8.90 J/cm | 16.7 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® FXD1413T PC Copolymer (Asia Pacific) Clear PC-siloxane copolymer with excellent processability, in special light diffusion colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may af.. |
|||
Izod Impact, Notched | 8.90 J/cm | 16.7 ft-lb/in | ASTM D256 |
IDI Composites 46-16 Thermoset Polyester, Molding Premium high strength electrical grade with excellent resistance to smoke generation, weathering, and corrosive environments.Data provided by the manufacturer. |
|||
Izod Impact, Notched | 8.90 J/cm | 16.7 ft-lb/in | ASTM D256 |
IDI Composites C-108 Thermoset Polyester, Molding Vinylester compounds in a range of strengths with superior corrosion resistance.Data provided by the manufacturer. |
|||
Izod Impact, Notched | 8.90 J/cm | 16.7 ft-lb/in | ASTM D256 |
IDI Composites E-205 Thermoset Polyester, Sheet ELECTRICAL - U.L. recognized (E53587). Versatile family of compounds designed to meet the most demanding electrical and electronic applications. Excellent dielectric properties and arc/track resista.. |
|||
Izod Impact, Notched | 8.90 J/cm | 16.7 ft-lb/in | ASTM-D256 |
Braskem GV0350 HDPE Blow Molding Polyethylene Copolymer HDPE GV0350 is a high-density polyethylene copolymer that has great molar mass, excellent chemical resistance, and high impact resistance and stiffness. It was developed for the blow-molding of larg.. |
|||
Izod Impact, Notched | 8.90 J/cm | 16.7 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® EXL1433T PC Copolymer Lexan* EXL1433T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding grade. This resin offers excellent low temperature (-30 C) ductility in combination with .. |