Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 8.65 J/cm | 16.2 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® EXL1414 PC Copolymer Lexan* EXL1414 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade. This resin offers extreme low temperature (-40 C) ductility in combination with excel.. |
|||
Izod Impact, Notched | 8.65 J/cm | 16.2 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® EXL1414 PC Copolymer (Asia Pacific) Lexan* EXL1414 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade. This resin offers extreme low temperature (-40 C) ductility in combination with excel.. |
|||
Izod Impact, Notched | 8.65 J/cm | 16.2 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® EXL1434 PC Copolymer Lexan* EXL1434 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade and is UV stabilized. This resin offers extreme low temperature (-40 C), exhibits exce.. |
|||
Izod Impact, Notched | 8.65 J/cm | 16.2 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® EXL1434 PC Copolymer (Asia Pacific) Lexan* EXL1434 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade and is UV stabilized. This resin offers extreme low temperature (-40 C), exhibits exce.. |
|||
Izod Impact, Notched | 8.65 J/cm | 16.2 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® EXL1434 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1434 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade and is UV stabilized. This resin offers extreme low temperature (-40 C), exhibits exce.. |
|||
Izod Impact, Notched | 8.65 J/cm | 16.2 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® EXL1444 PC Copolymer Lexan* EXL1444 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade suitable for FDA compliant applications. This resin offers extreme low temperature (-.. |
|||
Izod Impact, Notched | 8.65 J/cm | 16.2 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® EXL1444 PC Copolymer (Asia Pacific) Lexan* EXL1444 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade suitable for FDA compliant applications. This resin offers extreme low temperature (-.. |
|||
Izod Impact, Notched | 8.65 J/cm | 16.2 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® FXE1414 PC Copolymer Lexan* FXE1414 polycarbonate (PC) siloxane copolymer resin is a special effects fluorescent, medium flow opaque injection molding (IM) grade. This resin offers extreme low temperature (-40 C) ductil.. |
|||
Izod Impact, Notched | 8.65 J/cm | 16.2 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® EXL1414 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1414 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade. This resin offers extreme low temperature (-40 C) ductility in combination with excel.. |
|||
Izod Impact, Notched | 8.65 J/cm | 16.2 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® EXL1414H PC Copolymer Opaque PC-Siloxan copolymer with excellent processability. Medium flow, extreme low temperature ductile. Enhanced hydrolytic stability. Only available in black color. |
|||
Izod Impact, Notched | 8.65 J/cm | 16.2 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® EXL1414H PC Copolymer (Asia Pacific) Opaque PC-Siloxan copolymer with excellent processability. Medium flow, extreme low temperature ductile. Enhanced hydrolytic stability. Only available in black color. |
|||
Izod Impact, Notched | 8.65 J/cm | 16.2 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® EXL1414H PC Copolymer (Europe-Africa-Middle East) Opaque PC-Siloxan copolymer with excellent processability. Medium flow, extreme low temperature ductile. Enhanced hydrolytic stability. Only available in black color. |
|||
Izod Impact, Notched | 8.65 J/cm @Thickness 3.17 mm |
16.2 ft-lb/in @Thickness 0.125 in |
ASTM D-256 |
Axiall 2500 Rigid PVC, Extrusion Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Izod Impact, Notched | 8.65 J/cm @Thickness 3.17 mm |
16.2 ft-lb/in @Thickness 0.125 in |
ASTM D-256 |
Axiall 2501 Rigid PVC, Extrusion Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |