Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched = 8.541 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 8.541 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
16.00 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
0.25 mm notch; ASTM D256
LG Chemical Lupoy 1200-15 Polycarbonate Resin
Description: LUPOY PC 1200-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
Izod Impact, Notched 8.541 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
16.00 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
0.25 mm notch; ASTM D256
LG Chemical Lupoy 1201-15 Polycarbonate Resin
Description: LUPOY PC 1201-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
Izod Impact, Notched 8.541 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
16.00 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
0.25 mm notch; ASTM D256
LG Chemical Lupoy 1300-15 Polycarbonate Resin
Description: LUPOY PC 1300-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
Izod Impact, Notched 8.541 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
16.00 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
0.25 mm notch; ASTM D256
LG Chemical Lupoy 3010-15 Polycarbonate Resin
Description: LUPOY PC 3010-15 resin is designed for injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Character..
Izod Impact, Notched 8.541 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
16.00 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
0.25 mm notch; ASTM D256
LG Chemical Lupoy 3030-15 Polycarbonate Resin
Description: LUPOY PC 3030-15 resin is designed for injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Character..
Izod Impact, Notched 8.541 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
16.00 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
0.25 mm notch; ASTM D256
LG Chemical Lupoy NF1009F 15 Polycarbonate Resin
Description: LUPOY NF 1009F15, eco-friendly UL94 V0/2.0 mm, is designed for extrusion and injection molding products. It combines an excellent physical property balance of heat resistance, transpare..
Izod Impact, Notched 8.541 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
16.00 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
0.25 mm notch; ASTM D256
LG Chemical Lupoy 1200HP-15 Polycarbonate Resin
Description: LUPOY PC 1200HP-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
Izod Impact, Notched 8.541 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
16.00 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
0.25 mm notch; ASTM D256
LG Chemical Lupoy 1303-15 Polycarbonate Resin
Description: LUPOY PC 1303-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
Izod Impact, Notched 8.541 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
16.00 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
0.25 mm notch; ASTM D256
LG Chemical Lupoy 1303AH-15 Polycarbonate Resin
Description: LUPOY PC 1303AH-15 Tint Polycarbonate Resin is designed for injection molding of auto-headlamps. It exhibits an excellent physical property balance of heat resistance, transparency and ..
Copyright © lookpolymers.com All Rights Reserved