Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | >= 4.51 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
>= 8.45 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY GP5008A PC/ABS Description: Injection Molding, PC/ABS, General Purpose, High FlowApplication: Miscellaneous GoodsCAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical |
|||
Izod Impact, Notched | 4.51 J/cm @Thickness 3.17 mm |
8.45 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Unitika P-5001 Engineering Plastic P series resins are resins succeeding the characteristics of the neat polymer, U100, and improved in flowability and optical properties. Among many super engineering plastics, the resins are few tra.. |