Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 4.37 J/cm @Thickness 3.20 mm |
8.19 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
SABIC Innovative Plastics ULTEM 2310 PEI 30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. |
|||
Izod Impact, Notched | 4.37 J/cm @Thickness 3.20 mm |
8.19 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
SABIC Innovative Plastics ULTEM 2310 PEI (Asia Pacific) 30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. |
|||
Izod Impact, Notched | 4.37 J/cm @Thickness 3.20 mm |
8.19 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
SABIC Innovative Plastics ULTEM 2310F PEI 30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. US FDA Food Contact compliant in recognized colors. |
|||
Izod Impact, Notched | 4.37 J/cm @Thickness 3.20 mm |
8.19 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
SABIC Innovative Plastics ULTEM 4211 PEI 20% Glass fiber filled and PTFE filled, standard flow Polyetherimide (Tg 217C). ECO Conforming. |
|||
Izod Impact, Notched | 4.37 J/cm @Thickness 3.20 mm |
8.19 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
SABIC Innovative Plastics ULTEM 4211 PEI (Asia Pacific) 20% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming. |
|||
Izod Impact, Notched | 4.37 J/cm | 8.19 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL PPX PPX7110 PPE+PP PPE+PP blend. High Impact, Good Heat Resistance |
|||
Izod Impact, Notched | 4.37 J/cm | 8.19 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL PPX PPX7110 PPE+PP (Asia Pacific) PPE+PP blend. High Impact, Good Heat Resistance |