Mechanical Properties Metric English Comments
Izod Impact, Notched 0.270 - 8.17 J/cm
0.506 - 15.3 ft-lb/in
Average value: 1.31 J/cm Grade Count:11
Overview of materials for PET + PBT Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "PET + PBT Unreinforced". Each property range of values reported is minimum and maximum values of appropr..