Mechanical Properties Metric English Comments
Izod Impact, Notched 7.74 J/cm
14.5 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® EM1210 PC
Automotive interiors. Excellent heat/impact resistance and outstanding property retention over wide temperature range/severe automotive conditions
Izod Impact, Notched 7.74 J/cm
14.5 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® EM1210 PC (Asia Pacific)
Automotive interiors. Excellent heat/impact resistance and outstanding property retention over wide temperature range/severe automotive conditions
Izod Impact, Notched 7.74 J/cm

@Temperature -30.0 °C
14.5 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® EXL1414 PC Copolymer
Lexan* EXL1414 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade. This resin offers extreme low temperature (-40 C) ductility in combination with excel..
Izod Impact, Notched 7.74 J/cm

@Temperature -30.0 °C
14.5 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® EXL1414 PC Copolymer (Asia Pacific)
Lexan* EXL1414 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade. This resin offers extreme low temperature (-40 C) ductility in combination with excel..
Izod Impact, Notched 7.74 J/cm

@Temperature -30.0 °C
14.5 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® EXL1434 PC Copolymer
Lexan* EXL1434 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade and is UV stabilized. This resin offers extreme low temperature (-40 C), exhibits exce..
Izod Impact, Notched 7.74 J/cm

@Temperature -30.0 °C
14.5 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® EXL1434 PC Copolymer (Asia Pacific)
Lexan* EXL1434 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade and is UV stabilized. This resin offers extreme low temperature (-40 C), exhibits exce..
Izod Impact, Notched 7.74 J/cm

@Temperature -30.0 °C
14.5 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® EXL1434 PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1434 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade and is UV stabilized. This resin offers extreme low temperature (-40 C), exhibits exce..
Izod Impact, Notched 7.74 J/cm

@Temperature -30.0 °C
14.5 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® FXE1414 PC Copolymer
Lexan* FXE1414 polycarbonate (PC) siloxane copolymer resin is a special effects fluorescent, medium flow opaque injection molding (IM) grade. This resin offers extreme low temperature (-40 C) ductil..
Izod Impact, Notched 7.74 J/cm

@Thickness 3.17 mm
14.5 ft-lb/in

@Thickness 0.125 in
ASTM D256
Oxford Polymers PC C20-000 Clear PC
Product Description: Amorphous, Unreinforced Polycarbonate injection molding grade Processing and Delivery Form: Pellets and Injection MoldingAdditives: Pigment onlySpecial Characteristics: Easy fl..
Izod Impact, Notched 7.74 J/cm

@Temperature -30.0 °C
14.5 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® EXL1414 PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1414 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade. This resin offers extreme low temperature (-40 C) ductility in combination with excel..
Izod Impact, Notched 7.74 J/cm

@Temperature -30.0 °C
14.5 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® EXL1414H PC Copolymer
Opaque PC-Siloxan copolymer with excellent processability. Medium flow, extreme low temperature ductile. Enhanced hydrolytic stability. Only available in black color.
Izod Impact, Notched 7.74 J/cm

@Temperature -30.0 °C
14.5 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® EXL1414H PC Copolymer (Asia Pacific)
Opaque PC-Siloxan copolymer with excellent processability. Medium flow, extreme low temperature ductile. Enhanced hydrolytic stability. Only available in black color.
Izod Impact, Notched 7.74 J/cm

@Temperature -30.0 °C
14.5 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® EXL1414H PC Copolymer (Europe-Africa-Middle East)
Opaque PC-Siloxan copolymer with excellent processability. Medium flow, extreme low temperature ductile. Enhanced hydrolytic stability. Only available in black color.
Izod Impact, Notched 7.74 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
14.5 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Diamond Polymers DIAMALOY PC 1008 Impact Modified Polycarbonate
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Izod Impact, Notched 7.74 J/cm

@Temperature 22.8 °C
14.5 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Clariant PA131 Nylon 66, Highly Impact Modified
Data provided by Clariant Masterbatches
Izod Impact, Notched 7.74 J/cm

@Temperature 22.8 °C
14.5 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Clariant PA131G2GN-91 Green Nylon 66, Highly Toughened
Data provided by Clariant Masterbatches
Izod Impact, Notched 7.74 J/cm

@Temperature 22.8 °C
14.5 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Clariant Renol PA133 Nylon 66, Highly Impact Modified, Heat Stabilized, Lubricated
Data provided by Clariant Masterbatches
Izod Impact, Notched 7.74 J/cm

@Temperature 22.8 °C
14.5 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Clariant Renol PA133GN-109 Nylon 66, High Impact, Heat Stabilized, Lubricated
Data provided by Clariant Masterbatches
Izod Impact, Notched 7.74 J/cm
14.5 ft-lb/in
ASTM D256
Ashley Polymers Ashlene® P1043R Polycarbonate
A general purpose, injection molding grade, natural resin containing UV stabilizer.Data provided by the manufacturer
Izod Impact, Notched 7.74 J/cm
14.5 ft-lb/in
ASTM D256
Ashley Polymers Ashlene® P1044R Polycarbonate