Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 7.501 J/cm | 14.05 ft-lb/in | 73°F; ASTM D256 |
LyondellBasell Moplen EP/60 Bianco Polypropylene Copolymer Description: Moplen Coat EP/60 Bianco fractional melt flow, 1,200 MPa flexural modulus, extrusion grade polypropylene copolymer has a very good balance of properties and processability. Available in.. |
|||
Izod Impact, Notched | 7.501 J/cm | 14.05 ft-lb/in | 73°F; ASTM D256 |
LyondellBasell Hifaxâ„¢ RTA3263EUV Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ RTA3263EUV fractional melt flow, 1,500 MPa flexural modulus, UV-stabilized, mineral-filled, extrusion grade thermoplastic elastomeric olefin (TEO) resin has an excellent com.. |