Polymer Property : Izod Impact, Notched = 7.19 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 3.84 J/cm

@Thickness 3.20 mm
7.19 ft-lb/in

@Thickness 0.126 in
reverse notched; ASTM D 256
SABIC Innovative Plastics Ultem 2212 PEI
20% Milled glass filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched 3.84 J/cm

@Thickness 3.20 mm
7.19 ft-lb/in

@Thickness 0.126 in
reverse notched; ASTM D 256
SABIC Innovative Plastics Ultem 2212 PEI (Asia Pacific)
20% Milled glass filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region.
Izod Impact, Notched 3.84 J/cm

@Thickness 3.20 mm
7.19 ft-lb/in

@Thickness 0.126 in
ASTM D256
SABIC Innovative Plastics ULTEM 2212R PEI
20% Milled glass filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.
Izod Impact, Notched 3.84 J/cm

@Thickness 3.20 mm
7.19 ft-lb/in

@Thickness 0.126 in
ASTM D256
SABIC Innovative Plastics ULTEM 2212R PEI (Asia Pacific)
20% Milled glass filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.
Izod Impact, Notched 3.84 J/cm
7.19 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP VERTON RV00AES PA 66 (Asia Pacific)
LNP VERTON* RV00AES is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding.
Izod Impact, Notched 3.84 J/cm
7.19 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP VERTON RV00AES PA 66 (Europe-Africa-Middle East)
LNP VERTON* RV00AES is a compound based on PA 66 resin containing Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized.
Izod Impact, Notched 3.84 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
7.19 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Diamond Polymers ABS 7401 Injection Molding Grade, Extra High Impact
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Izod Impact, Notched 3.84 J/cm
7.19 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP VERTON RV00AES PA 66
LNP VERTON* RV00AES is a compound based on Nylon 66 resin containing 50% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, Structural.
Izod Impact, Notched 3.84 J/cm
7.19 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP VERTON RX06422 PA 66
LNP VERTON* RX06422 is a compound based on Nylon 66 resin containing 50% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, UV Stabilized, Structural.
Izod Impact, Notched 3.84 J/cm
7.19 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP VERTON RX06422 PA 66 (Asia Pacific)
LNP VERTON* RX06422 is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding.