Mechanical Properties Metric English Comments
Izod Impact, Notched 7.16 J/cm
13.4 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® BFL2000B PC (Asia Pacific)
Lexan BFL2000B resin is a Br- & Cl-free FR polycarbonate resin featuring high flow with balanced impact. It is available only in dark colors.
Izod Impact, Notched >= 7.16 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
>= 13.4 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
LG Chemical LUPOY GN1006FM PC, Halogen Free, Flame Retardant, Transparency
Description: Injection Molding, PC, Halogen Free Flame Retardant, TransparencyApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2Information provided by LG Chemical
Izod Impact, Notched >= 7.16 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
>= 13.4 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
LG Chemical LUPOY GN1006FMR PC, Halogen Free, Flame Retardant, Transparency