Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 6.67 J/cm @Temperature -30.0 °C |
12.5 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® EXL1112 PC Copolymer Lexan* EXL1112 polycarbonate (PC) siloxane copolymer resin is a high flow opaque injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with excellent .. |
|||
Izod Impact, Notched | 6.67 J/cm @Temperature -30.0 °C |
12.5 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® EXL1112 PC Copolymer (Asia Pacific) Lexan* EXL1112 polycarbonate (PC) siloxane copolymer resin is a high flow opaque injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with excellent .. |
|||
Izod Impact, Notched | 6.67 J/cm @Temperature -30.0 °C |
12.5 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® EXL1112 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1112 polycarbonate (PC) siloxane copolymer resin is a high flow opaque injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with excellent .. |
|||
Izod Impact, Notched | 6.67 J/cm @Temperature -30.0 °C |
12.5 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® EXL1132 PC Copolymer Lexan* EXL1132 polycarbonate (PC) siloxane copolymer resin is a high flow, UV stabilized injection molding grade. This resin offers good low temperature (-20 C) ductility in combination with high fl.. |
|||
Izod Impact, Notched | 6.67 J/cm @Temperature -30.0 °C |
12.5 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® EXL1132 PC Copolymer (Asia Pacific) Lexan* EXL1132 polycarbonate (PC) siloxane copolymer resin is a high flow, UV stabilized injection molding grade. This resin offers good low temperature (-20 C) ductility in combination with high fl.. |
|||
Izod Impact, Notched | 6.67 J/cm @Temperature -30.0 °C |
12.5 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® EXL1132 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1132 polycarbonate (PC) siloxane copolymer resin is a high flow, UV stabilized injection molding grade. This resin offers good low temperature (-20 C) ductility in combination with high fl.. |
|||
Izod Impact, Notched | 6.67 J/cm | 12.5 ft-lb/in | Lengthwise; ASTM D256 |
G-9 Fiberglass Melamine Laminate Sheet This material is very hard, flame resistant, and has excellent electrical properties. G-9 has high arc and heat resistance and is recommended for humid environments. It is used for switch board pane.. |
|||
Izod Impact, Notched | 6.67 J/cm | 12.5 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® 3706 PBT+PC Impact modified PBT+PC resin. Outdoor enclosure. Not available in all colors. |
|||
Izod Impact, Notched | 6.67 J/cm | 12.5 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Xenoy® 1731 PBT+PC Impact/chemical resistant. UV-Stabilized. Excellent physical property retention in automotive exteriors and OVAD. |
|||
Izod Impact, Notched | 6.67 J/cm | 12.5 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Xenoy® 1731 PBT+PC (Asia Pacific) Impact/chemical resistant. UV-Stabilized. Excellent physical property retention in automotive exteriors and OVAD. |
|||
Izod Impact, Notched | 6.67 J/cm @Temperature -30.0 °C |
12.5 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Xenoy® 6620 PBT+PC PBT+PC, Unreinforced, impact modified thermoplastic alloy. Outstanding impact at low temperature |
|||
Izod Impact, Notched | 6.67 J/cm @Temperature -30.0 °C |
12.5 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Xenoy® 6620U PBT+PC PBT+PC, Unfilled, Impact Modified, UV stabilized. Outstanding low temperature impact performance and chemical resistance. |
|||
Izod Impact, Notched | 6.67 J/cm | 12.5 ft-lb/in | 73°F, 0.125 in.; ASTM D256 |
Star Plastics PC/PBT7804 Molding Grade PC/PBT Information provided by Star Plastics, Inc. |
|||
Izod Impact, Notched | 6.67 J/cm | 12.5 ft-lb/in | 73°F, 0.125 in.; ASTM D256 |
Star Plastics PC/PBT7820 Molding Grade PC/PBT Information provided by Star Plastics, Inc. |
|||
Izod Impact, Notched | 6.67 J/cm | 12.5 ft-lb/in | 73°F, 0.125 in.; ASTM D256 |
Star Plastics PC/PBTQX7008 Molding Grade PC/PBT Information provided by Star Plastics, Inc. |
|||
Izod Impact, Notched | 6.67 J/cm @Thickness 3.17 mm |
12.5 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Total 54050 HDPE, blow molding Applications: 55-gallon shipping containers, open-top drums, industrial tanks, agricultural chemical tanks. Blow Molding Stock Temperature 380 – 450 ºF Extrusion melt temperature 400 - 480ºFInfor.. |
|||
Izod Impact, Notched | 6.67 J/cm | 12.5 ft-lb/in | 73°F; ASTM D256 |
CPC - Vycom PROTEC® Copolymer Polypropylene (CPP) Protec CP is one of various types of "impact copolymers"—a rapidly growing segment of the thermoplastic sheet market. In contrast to homopolymer polypropylene (which involves the polymerization of .. |
|||
Izod Impact, Notched | 6.67 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
12.5 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D-256 |
Axiall 8302 Rigid PVC, Extrusion & Molding Georgia Gulf 8302 is a clear rigid PVC pellet compound suited for applications where transparency is important in a high sunlight environment. It can be used for exterior transparent profiles such .. |
|||
Izod Impact, Notched | 6.67 J/cm | 12.5 ft-lb/in | Lengthwise; ASTM D256 |
G-5 Fiberglass Melamine Laminate Sheet This material is very hard, flame resistant, and has excellent electrical properties. G-5 has high arc and heat resistance. It used for switch board panels, arc barriers, circuit breaker parts, and .. |