Polymer Property : Izod Impact, Notched = 6.60 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 6.60 J/cm
12.4 ft-lb/in
ASTM D256
SPS Guang Zhou POLLITEâ„¢ 1001(+) Flame-retarded Polycarbonate
Characteristic: Good flame retardance, high notched impact strength, high heat resistanceApplications: Computer, E/E applianceInformation Provided by SPS (Guang Zhou) Ltd.
Izod Impact, Notched 6.60 J/cm
12.4 ft-lb/in
ASTM D256
SABIC Innovative Plastics XYLEX X7300 PC+POLYESTER
PC+POLYESTER unreinforced alloy. High flow, chemically resistant with excellent optical quality. UV-stabilized.
Izod Impact, Notched 6.60 J/cm
12.4 ft-lb/in
ASTM D256
SABIC Innovative Plastics XYLEX X7300 PC+POLYESTER (Asia Pacific)
PC+POLYESTER unreinforced alloy. High flow, chemically resistant with excellent optical quality. UV-stabilized.
Izod Impact, Notched 6.60 J/cm
12.4 ft-lb/in
ASTM D256
SABIC Innovative Plastics XYLEX X7300 PC+POLYESTER (Europe-Africa-Middle East)
PC+POLYESTER unreinforced alloy. High flow, chemically resistant with excellent optical quality. UV-stabilized.
Izod Impact, Notched 6.60 J/cm
12.4 ft-lb/in
ASTM D256
SABIC Innovative Plastics XYLEX X7300CL PC+POLYESTER
PC+ POLYESTER unreinforced alloy developed for optical or lense market. Chemical resistance.
Izod Impact, Notched 6.60 J/cm
12.4 ft-lb/in
ASTM D256
SABIC Innovative Plastics XYLEX X7300CL PC+POLYESTER (Asia Pacific)
PC+ POLYESTER unreinforced alloy developed for optical or lense market. Chemical resistance.
Izod Impact, Notched 6.60 J/cm
12.4 ft-lb/in
ASTM D256
SABIC Innovative Plastics XYLEX X7300CL PC+POLYESTER (Europe-Africa-Middle East)
PC+ POLYESTER unreinforced alloy developed for optical or lense market. Chemical resistance.
Izod Impact, Notched 6.60 J/cm

@Temperature 23.0 °C
12.4 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Xylex X7300OQ PC+POLYESTER (Asia Pacific)
PC+ POLYESTER unreinforced alloy developed for optical or lense market. High flow with good impact and excellent optical quality.This data was supplied by SABIC-IP for the Asia Pacific region.
Izod Impact, Notched 6.60 J/cm

@Temperature 23.0 °C
12.4 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Xylex X7300OQ PC+POLYESTER (Europe-Africa-Middle East)
PC+ POLYESTER unreinforced alloy developed for optical or lense market. High flow with good impact and excellent optical quality.This data was supplied by SABIC-IP for the Europe-Africa-Middle East..